1.4571 X6CrNiMoTi17-12-2 Austenitic Stainless Steel
Introduce
Grade 1.4571 is an austenitic titanium stabilized stainless steel. 1.4571/316Ti got a good corrosion resistance as well as good mechanical properties. This steel grade is still often being used in Germany.Internationally 1.4404/316L is offten being used instead since itts corrosion resistance is the same but 1.4404 is way simpler to process.
Our supply size:
Diameter : 80 to 600 mm ;
Length : 1000 to 9000 mm ;
Our advantage:
- High Quality, Reasonable Price
- Over 40 Years Experience
- ISO NQA Certificated Factory
- Worldwide shipping
- Emergency Orders and Fast Delivery
Equivalent grades of steel X6CrNiMoTi17-12-2 (1.4571)
| EU | USA | Germany | Japan | France | England | Italy |
| EN | – | DIN,WNr | JIS | AFNOR | BS | UNI |
| X6CrNiMoTi17-12-2 | 316Ti | X10CrNiMoTi18-10 | 316Ti | Z6CNDT17-12 | 320S31 | X6CrNiMoTi17-12 |
Chemical composition % of steel X6CrNiMoTi17-12-2 (1.4571): EN 10088-2-2005
| C | Si | Mn | Ni | P | S | Cr | Mo | Ti |
| max 0.08 | max 1 | max 2 | 10.5 – 13.5 | max 0.045 | max 0.015 | 16.5 – 18.5 | 2 – 2.5 | max 0.7 |
Mechanical properties of steel X6CrNiMoTi17-12-2 (1.4571)
| Rm – Tensile strength (MPa) (+A) | 500-700 |
| Rm – Tensile strength (MPa) (+AT) | 500-730 |
| Rm – Tensile strength (MPa) (+AT+C) | 810-850 |
| Rp0.2 0.2% proof strength (MPa) (+A) | 200-240 |
| Rp0.2 0.2% proof strength (MPa) (+AT) | 190-210 |
Smelting Option
1 EAF: Electric Arc Furnace
2 EAF+LF+VD: Refined-smelting and vacuum degassing
3 EAF+ESR: Electro Slag Remelting
4 EAF+PESR: protective atmosphere Electro Slag Remelting
5 VIM+PESR: Vacuum induction melting
Forming Option
1 Hot rolling process
2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging
Heat-treatment Option
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
Surface Option
1 Black Surface
2 Grounded: Bright but rough ; Not precision
3 Machining for plate: Bright and precision; Little turning scar
4 Peeled/Turned: Bright and precision; Little turning scar
5 Polished: Very Bright and precision size; Not turning scar
Other Services
1 Cutting: Small pieces
2 CNC Machine: Produce as your drawing
3 Package: Bare/Nylon/Canvas/Wooden
4 Payment:T/T, L/C, O/A(request credit)
5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)
Mill test certificate
EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.