manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Nickel 270 UNS N02270 2.4050 High Purity Nickel Alloy

Nickel 270 UNS N02270 2.4050 High Purity Nickel Alloy

Nickel 270 UNS N02270 2.4050 High Purity Nickel Alloy

With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

 

Description

A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for electrical resistance thermometers.

 

Nickel 270 alloy is an unalloyed high purity nickel alloy that has high ductility and low base hardness. It is made by powder metallurgy. It contains 99.8% nickel in addition to traces of minor elements. It is essentially free from non-metallic inclusions.

 

EQUIVALENT STANDARDS

ASTM AISI EN DIN UNS
Alloy 270 Nickel 270 2.405 Ni99.8 N02270

 

CHEMICAL PROPERTIES

Element Min % Max %
Ni + Co 99 –
Cu – 0.01
Fe – 0.05
Mn – 0.003
C – 0.05
S – 0.003
Ti – 0.005
Mg – 0.005
Si – 0.005
Al – 0.005

 

MECHANICAL PROPERTIES

YSRp02 TSRm A HRB
110 340 50 65

 

Density 8.89 g/cn? 0321 lb/in3
Melting Point 1454 °C 2650 °F
Coefficient of Expansion 13.3 pm/m°C(20- 100°C) 7.4xl06in/in°F (70-212 °F)
Modulus of Rigidity 82 kN/mm2 11893 ksi
Modulus of Elasticity 207 kN/mm2 30000 ksi

 

Properties
Condition Approx, tensile strength Approx, operating temperature
N/mm2 ksi
Annealed 300 – 450 44-65 Tensile strength and elongation drop significantly at temperatures above 315 °C (600 °F). Service temperature is dependent on environment, load and size range.
Hard Drawn 600 – 800 87-116

The above tensile strength ranges are Typical. If you require different please ask.

 

Key Features

Nickel® 270 offers the following key features:

High purity grade of nickel that is made by powder metallurgy.

 

Applications of Nickel 270

Fluorescent Light Components

Electronic Cathodes or Anodes

Resistance Thermometers

Electrical Resistance Thermometers

Components for Hydrogen Thyratrons

Electrical and Electronic Components

 

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x