S47010 15Cr12WMoV 1Cr12W1MoV Stainless Steel For Steam Turbine Blade

S47010 15Cr12WMoV 1Cr12W1MoV Stainless Steel For Steam Turbine Blade

S47010 15Cr12WMoV 1Cr12W1MoV Stainless Steel For Steam Turbine Blade

Supplying dimension

Round bar from         30mm to 600mm Diameter

Flat and square bar from  30mm to 500mm Width

8mm to 300mm Thickness

*accept special shape

 

Forming option

Hot rolling or hot forged

 

Smelting process

EAF →VD→LF→ESR Electro-Slag Remelting

 

Surface option

Black

Grinding

Rough turned

Peeled

Polished

 

Quality

UT, size and surface for each pcs

Macrostructure

Ferritic Metallographic

Grain size

Nonmetallic inclusion

Etch test of tower sample

 

Delivery condition and hardness

Annealed or high temperature temper

Annealed high temperature temper Hardness
800 to 900 Celsius, slow 700 to 770 Celsius, fast Max 223 HBW

*Accept +QT delivery condition

 

Equivalent Grade

Chinese UNS Chinese New Grade Chinese Old Grade
S47010 15Cr12WMoV 1Cr12W1MoV

 

Chemical component

C Si Mn P S Ni Cr Cu Mo V W
0.12 to 0.18 Max 0.50 0.50 to 0.90 Max 0.030 Max 0.020 0.40 to 0.80 11.00 to 13.00 Max 0.30 0.50 to 0.70 0.15 to 0.30 0.70 to 1.10

 

Mechanical property and heat treatment

Type Quench temperature Temper temperature Specified Plastic Elongation Strength Tensile strength Elongation Reduction Impact Hardness
1 1000 to 1050 Celsius, air, oil 680 to 740 Celsius, air Min 590 Mpa Min 735 Mpa Min 15 % Min 45% Min 27 KJ 229 to 277 HBW
2 1000 to 1050 Celsius, oil 660 to 700 Celsius, air Min 635 Mpa Min 785 Mpa Min 15 % Min 45% Min 27 KJ 248 to 293 HBW

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists