Excellent products and services, customer recognition
Order Exhibition
Project location:Italy
Product:RING, HOLLOW, SHEET, BAR
Standard and material:C276
Inquiry time:2022.08
Order time:2022.08
Shipping time:2022.10
Arrival time:2022.11
Starting from the heart is the consistent purpose of Fushun. In the future, we will continue to solve various service requirements of customers by our heart.
Our client is one of Europe’s largest producers of hydrofluoric acid and fluoroderivatives. They provides through its plants in Porto Marghera, from which major manufacturers operating in the fluoropolymer, refrigerant, pharmaceutical, agrochemical, electronics, metallurgy, fertilizer, construction and other industries are supplied.
Supplied Size:
| No. | Product Name | Material NO. | Dimensions | Weight
(kg/each) |
QTY | |||
| OD | ID | Height | PCS | KGS | ||||
| (mm) | (mm) | (mm) | ||||||
| 1 | RING | C276 | 1610 | 1080 | 60 | 617 | 1 | 617 |
| 2 | HOLLOW BAR | C276 | 280 | 160 | 125 | 47.2 | 1 | 47.2 |
| 3 | SHEET DISC | C276 | 700 | / | 30 | 112 | 1 | 112 |
| SUB TOTAL | 3 | 776.2 | ||||||
| No. | Product Name | Material NO. | Dimensions | Weight
(kg/each) |
QTY | |||
| DIA | Length | PCS | KGS | |||||
| (mm) | (mm) | |||||||
| 4 | ROUND BAR | C276 | 310 | 170 | 115 | 1 | 115 | |
| 5 | C276 | 100 | 100 | 7.2 | 1 | 7.2 | ||
| 6 | C276 | 180 | 35 | 8.4 | 1 | 8.4 | ||
| 7 | C276 | 180 | 70 | 16.4 | 1 | 16.4 | ||
| 8 | C276 | 180 | 80 | 18.7 | 2 | 37.4 | ||
| 9 | C276 | 204 | 70 | 20.8 | 1 | 20.8 | ||
| 10 | C276 | 204 | 55 | 16.5 | 1 | 16.5 | ||
| 11 | C276 | 230 | 80 | 30.4 | 2 | 60.8 | ||
| SUB TOTAL | 10 | 282.5 | ||||||
| No. | Product Name | Material NO. | Dimensions | Weight
(kg/each) |
QTY | |||
| Width | Thickness | Length | PCS | KGS | ||||
| (mm) | (mm) | (mm) | ||||||
| 12 | SHEET PLATE | C276 | 400 | 30 | 750 | 80.4 | 1 | 80.4 |
| 13 | C276 | 1000 | 12 | 2000 | 216.4 | 1 | 216.4 | |
| 14 | C276 | 450 | 15 | 1548 | 93.6 | 1 | 93.6 | |
| 15 | C276 | 2000 | 15 | 2000 | 537 | 1 | 537 | |
| 16 | C276 | 820 | 15 | 3345 | 367.4 | 1 | 367.4 | |
| 17 | C276 | 480 | 25 | 2277 | 245.5 | 2 | 491 | |
| 18 | C276 | 1350 | 25 | 2468 | 756 | 1 | 756 | |
| 19 | C276 | 1500 | 30 | 1000 | 403.13 | 3 | 1209.40 | |
What is C276?
C276 (UNS N10276) is a cold hardened nickel-based alloy intended for the most extreme well conditions up to 450°F.
In addition to its exceptional corrosion resistance under the most severe conditions, higher strengths may be achieved with C276 than other nickel alloys. It is therefore used for downhole tubular components, packers, and other subsurface equipment under the most extreme environmental conditions found in high-pressure, high-temperature (HPHT) wells, saltwater Injection wells, and Acid Gas Injection (AGI) wells. However, all environmental factors, including H2S, CO2 , temperature, pH, and chloride concentration, should be considered before final material selection.
The alloy is classified in MR0175/ISO15156 as a type 4e alloy, with no restrictions to a partial pressure of H2S below 400°F and resistant to 1000 psi H2S at 450°F.
Hastelloy C276 alloy (UNS N10276) was the first wrought, nickel-chromium- molybdenum material to alleviate concerns over welding (by virtue of extremely low carbon and silicon contents). As such, it was widely accepted in the chemical process and associated industries.
ALSO KNOWN AS
- C-276
- SMC276®
- INCONEL® Alloy C-276
- Hastelloy® C-276
- W.Nr. 2.4819
Applications
Typical chemical process industry (CPI) applications include reactors, heat exchangers, and columns, marine hardware, Chemical processing components Agrichemical and petrochemical production.