HS0-4-1,1.3325, High-speed Tool Steel
Introduce
| Grade : | HS0-4-1 |
| Number: | 1.3325 |
| Classification: | High-speed tool steel |
| Standard: | EN ISO 4957: 2000 Tool steels |
Chemical composition % of steel HS0-4-1 (1.3325): EN 4957-2000
| C | Si | Mn | P | S | Cr | Mo | V |
| 0.77 – 0.85 | max 0.65 | max 0.4 | max 0.03 | max 0.03 | 3.9 – 4.4 | 4 – 4.5 | 0.9 – 1.1 |
Mechanical properties of steel HS0-4-1 (1.3325)
| Brinell hardness (HB): (+A) | 262 |