Thank You for Choosing H13 D6 M2 D2: Appreciating Your Trust in our High-Temperature Tool Steel
We, Fushun are thrilled to have the opportunity to provide client with high-quality, reliable tool steel for client manufacturing needs.
Client decision to choose our products is a testament to the trust you have in our company and our ability to meet your needs. We are honored to have earned client business and look forward to continuing our partnership with client in the future.
As you know, H13, D6, D2, and M2 steel are all exceptional materials that are widely recognized for their toughness, durability, and ability to hold a sharp edge. We are confident that you will find these materials to be of the highest quality and perfectly suited to client needs.
Thank you again for your business and for choosing FUSHUN as your trusted provider of tool steel. We look forward to working with you and helping you achieve your manufacturing goals.
DESCRIPTION OF GOODS: Tool Steel Round Bars & Plates
| S.R. No. | Quality Standard | Steel Grade | Delivery Condition | Surface Condition | Dimensions(mm) | QTY | ||||
| Diameter | Length | PC | PKG | N.W(KG) | G.W(KG) | |||||
| 1 | ASTM A681 | H13 | Annealed | Peeled | 15 | Random Length | 1 | 1 | 535 | 535 |
| 2 | ASTM A681 | H13 | Annealed | 25 | 1 | 1 | 455 | 455 | ||
| 3 | ASTM A681 | H13 | Annealed | 30 | 1 | 1 | 183 | 183 | ||
| 4 | ASTM A681 | H13 | Annealed | 40 | 1 | 1 | 627 | 627 | ||
| 5 | ASTM A681 | H13 | Annealed | 45 | 1 | 1 | 640 | 640 | ||
| 6 | ASTM A681 | H13 | Annealed | 50 | 1 | 1 | 952 | 952 | ||
| 7 | ASTM A681 | H13 | Annealed | 55 | 1 | 1 | 1107 | 1107 | ||
| 8 | ASTM A681 | H13 | Annealed | 60 | 1 | 1 | 1161 | 1161 | ||
| 9 | ASTM A681 | H13 | Annealed | 65 | 1 | 1 | 1049 | 1049 | ||
| 10 | ASTM A681 | H13 | Annealed | Grinded | 70 | 9 | 1 | 1046 | 1046 | |
| 11 | ASTM A681 | H13 | Annealed | 75 | 8 | 1 | 1052 | 1052 | ||
| 12 | ASTM A681 | H13 | Annealed | 80 | 7 | 1 | 1060 | 1060 | ||
| 13 | ASTM A681 | H13 | Annealed | 85 | 7 | 1 | 1132 | 1132 | ||
| 14 | ASTM A681 | H13 | Annealed | 90 | 4 | 1 | 1034 | 1034 | ||
| 15 | ASTM A681 | H13 | Annealed | 100 | 4 | 1 | 1038 | 1038 | ||
| 16 | ASTM A681 | H13 | Annealed | 115 | 3 | 1 | 1082 | 1082 | ||
| 17 | ASTM A681 | H13 | Annealed | 130 | 2 | 1 | 1094 | 1094 | ||
| 18 | ASTM A681 | H13 | Annealed | 140 | 2 | 1 | 1122 | 1122 | ||
| 19 | ASTM A681 | H13 | Annealed | 150 | 2 | 1 | 1366 | 1366 | ||
| 20 | ASTM A681 | D6 | Annealed | Grinded | 75 | 8 | 1 | 840 | 840 | |
| 21 | ASTM A681 | D6 | Annealed | 90 | 8 | 1 | 1924 | 1924 | ||
| 22 | ASTM A681 | D6 | Annealed | 100 | 7 | 1 | 1742 | 1742 | ||
| 23 | ASTM A681 | D6 | Annealed | 130 | 3 | 1 | 1316 | 1316 | ||
| 24 | ASTM A681 | D6 | Annealed | 150 | 2 | 1 | 1110 | 1110 | ||
| 25 | ASTM A681 | D6 | Annealed | 180 | 1 | 616 | 616 | |||
| 26 | ASTM A600 | M2 | Annealed | Peeled | 20 | 1 | 1 | 308 | 308 | |
| 27 | ASTM A600 | M2 | Annealed | 22 | 1 | 216 | 216 | |||
| 28 | ASTM A600 | M2 | Annealed | 25 | 1 | 512 | 512 | |||
| 29 | ASTM A600 | M2 | Annealed | 30 |
Random Length |
1 | 1 | 508 | 508 | |
| 30 | ASTM A600 | M2 | Annealed | 35 | 1 | 536 | 536 | |||
| 31 | ASTM A600 | M2 | Annealed | 40 | 1 | 536 | 536 | |||
| 32 | ASTM A600 | M2 | Annealed | 45 | 1 | 1 | 508 | 508 | ||
| 33 | ASTM A600 | M2 | Annealed | 50 | 1 | 498 | 498 | |||
| 34 | ASTM A600 | M2 | Annealed | 60 | 1 | 378 | 378 | |||
| 35 | ASTM A600 | M2 | Annealed | 65 | 1 | 1 | 530 | 530 | ||
| 36 | ASTM A600 | M2 | Annealed | 75 | 1 | 280 | 280 | |||
| 37 | ASTM A681 | O1 | Annealed | Black | 15,0 x 600 | 2 | 2 | 647 | 647 | |
| 38 | ASTM A681 | H13 | Annealed | Black | 300X 600 | 1 | 1 | 3522 | 3522 | |
| 39 | ASTM A600 | M2 | Annealed | Black | 100 x 200 | 1 | 1 | 354 | 354 | |
| 40 | / | AISI420 | Annealed | Black | 300 X 600 | 1 | 1 | 4044 | 4044 | |
| 41 | ASTM A681 | D2 | Annealed | Black | 300 x 600 | 1 | 1 | 4858 | 4858 | |
| 42 | ASTM A681 | O1 | Annealed | Black | 300 x 600 | 1 | 1 | 5286 | 5286 | |
| Total | 104 | 35 | 48804 | 48804 | ||||||
Here’s an order introduction to H13 steel, D6 steel, M2 steel, and D2 steel:
H13 steel is a type of hot-work tool steel that is known for its excellent combination of toughness, wear resistance, and high-temperature strength. It is commonly used in applications such as die casting, extrusion, and forging, as well as in the manufacture of plastic molds and other high-temperature tools. H13 steel is highly regarded for its ability to maintain its hardness and strength even at elevated temperatures, making it a popular choice for applications that involve repeated heating and cooling cycles.
D6 steel, also known as AISI D6, is a high-carbon, high-chromium tool steel that is often used for cold-work applications such as blanking and forming dies, thread rolling dies, and punches. D6 steel is known for its excellent wear resistance and toughness, as well as its ability to hold a sharp cutting edge.
M2 steel, also known as high-speed steel (HSS), is a type of tool steel that is designed for use in high-speed cutting applications. It contains a high concentration of tungsten, molybdenum, and vanadium, which give it excellent wear resistance, toughness, and heat resistance. M2 steel is commonly used in applications such as drills, taps, end mills, and other cutting tools.
D2 steel, also known as AISI D2 or DIN 1.2379, is a high-carbon, high-chromium tool steel that is commonly used for cold-work applications such as blanking and forming dies, thread rolling dies, and punches. D2 steel is known for its high wear resistance and toughness, as well as its ability to maintain a sharp cutting edge for extended periods of use.
All of these types of tool steel are highly regarded for their durability, toughness, and ability to hold a sharp edge. The specific type of tool steel that is chosen for a particular application will depend on a variety of factors, including the specific cutting or shaping application, the desired level of wear resistance and toughness, and the available manufacturing processes.