AISI A8 MOD Cold Work Tool Steel
1: AISI A8 MOD steel introduction
A8-mod is a modified version of AISI A8. It’s a conventional cold work tool steel, with a medium carbon content and alloyed with chromium, molybdenum and vanadium. This steel is an improved steel of A8 steel, with good hardenability, toughness, heat treatment dimensional stability. Suitable for punches and cold forging dies with hardness requirements of 55-60 HRC. In addition, it is suitable for manufacturing non-metallic materials due to good hardness, wear resistance and toughness.
Cutting:
Precision cutting to standard dimensions
Custom cutting according to client specifications
Cold Work Tool Steel Dimensions
We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.
| Product Form | Specifications |
|---|---|
| Forged Round Bar | Dia. up to 1200mm |
| Forged Flat Bar | Thickness 100-600mm, Width 300-2000mm |
| Rolled Round Bar | Dia. 10-200mm |
| Hot Rolled Plate | Thickness 1-100mm, Width 60-1600mm |
2: AISI A8 MOD Steel equivalent
| Country | China | Japan | Germany | USA | UK |
| Standard | GB/T 1299 | JIS G4404 | DIN EN ISO4957 | ASTM A681 | BS 4659 |
| Grade | / | / | / | A8 MOD | / |
3: AISI A8 MOD steel chemical composition
| Grade | C | Mn | P | S | Si | Cr | V | Mo |
| A8 MOD | 0.50 | 0.30 | 0.03 | 0.03 | 0.95 | 8.01 | 0.50 | 1.45 |
4: AISI A8 MOD steel mechanical properties
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT.
6. AISI A8 MOD Tool Steel Heat Treatment
Annealing
Slowly heat to 870 – 890 ℃ , then slowly Cool to 500 ℃ in heat treatment furnace. Then frosty in make public. After annealing hardness HBS: 229 Max
Quenching
Quenching temperature / ℃ | outlet air cooling, oil cooling or air cooling : 1000 – 1050
Quenching hardness : 59-62 HRC
Tempering
Tempering temperature / ℃ : 150 – 320
After tempering hardness HRC or future: 53 – 60
7: Delivery condition
For hot forged or hot rolled bar, usually the delivery condition is hot forged or rolled, annealed, rough turned.
For hot forged plate, usually the delivery condition is hot forged, annealed, milled surface.
For hot rolled plate, usually the delivery condition is hot rolled, annealed, black surface.