56SiCr7 1.7106 Bright Spring Steel Rod

56SiCr7 1.7106 Bright Spring Steel Rod

Cold Finished Round Steel - Cold DrawnRolled

Cold Finished Round Steel – Cold DrawnRolled

 

We can supply bright steel rod after +QT heat treatment.

 

Ground bright steel

We supply ground bright steel according to DIN EN 10278 to tolerance class IT 6.

 

Turned/Peeled bright steel

We supply peeled round material according to DIN EN 10278 in tolerance class IT 11 or IT 9. Other tolerances can be supplied upon request.

 

Polished bright steel

The first stage, if the material is unfinished, starts with a rough abrasive (perhaps 60 or 80 grit) and each subsequent stage uses a finer abrasive, such as 120, 180, 220/240, 320, 400 and higher grit abrasives, until the desired finish is achieved.

 

Drawn bright steel

Drawn bright steel is produced from hot-rolled steel bar or wire by chipless drawing.

We supply drawn bright steel in a wide range of cross-sectional shapes according to DIN EN 10278 in tolerance class IT 11 or IT 9.

 

Chemical composition

Name Number C Si Mn P S Cr
max. max.
56SiCr7 1.7106 0,52-0,60 1,60-2,00 0,70-1,00 0,025 0,025 0,20-0,45

 

Mechanical Properties

Grade Condition Yield strength min [MPa] Tensile strength [MPa] Elongation A [%]
56SiCr7 EN10089 +QT 1350 1500- 1800 6

 

Transformation temperatures

Temperature °C
MS 265
AC1 770
AC3 821

 

Other properties (typical values)

Youngs module (GPa) Poisson´s ratio (-) Shear module (GPa) Density (kg/m3)
210 0.3 80 7800
Average CTE 20-300°C (µm/m°K) Specific heat capacity 50/100°C (J/kg°K) Thermal conductivity Ambient temperature (W/m°K) Electrical resistivity Ambient temperature (µΩm)
12 460 – 480 40 – 45 0.20 – 0.25

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x