Product Description

FUSHUN METAL’s 41CrAlMo7-10 Steel is a premium chromium-aluminum-molybdenum nitriding steel offering an exceptional combination of high core strength, excellent nitriding response, good toughness, and superior wear resistance in nitrided condition. With a carefully engineered chemical composition featuring optimized levels of aluminum (0.7-1.0%), chromium (1.5-1.8%), and molybdenum (0.25-0.35%), our 41CrAlMo7-10 delivers outstanding performance in demanding applications requiring both high surface hardness and good core strength. Available in multiple forms including round bars, flat bars, plates, forgings, and custom shapes, this versatile steel is ideal for applications in heavy-duty gears, camshafts, crankshafts, highly stressed machine components, forming and punching tools, and other applications where both wear resistance and fatigue strength are essential. The aluminum content enables the formation of extremely hard aluminum nitrides during nitriding, producing surface hardness up to 1000-1100 HV without requiring conventional quench and temper heat treatment. Each product undergoes comprehensive quality control to ensure consistent properties, precise dimensions, and superior surface quality for reliable performance in critical industrial applications.

Equivalent Steel Grades

41CrAlMo7-10 is part of a family of nitriding steels with the following equivalent grades in different standards:

Standard Designation Comparable Grades
EN 41CrAlMo7-10 31CrAlMo7-10, 34CrAlMo5-10, 34CrAlNi7-10
DIN 1.8509 1.8506 (31CrAlMo7-10), 1.8507 (34CrAlMo5-10), 1.8550 (34CrAlNi7-10)
AISI/SAE Similar to 8620H (modified) Nitralloy N, Nitralloy 135M
British BS 905M39 722M24, EN41B
Japanese JIS SACM645 SACM645, SACM940
Chinese GB 38CrAlMo 40CrAlMo, 38CrMoAl
Russian GOST 38KH2MYuA 38KH2MYUA, 38KH2MYuA
Italian UNI 40CrAlMo7-10 38CrAlMo7-10

Available Product Forms and Dimensions

FUSHUN METAL offers 41CrAlMo7-10 Nitriding Steel in a wide range of forms to meet diverse application requirements:

Round Bar Specifications

Diameter (mm) Standard Length (mm) Tolerance Surface Condition
10 – 30 3000, 6000, Fixed or Random h9, h10, h11, k12 Black, Peeled, Turned, Ground, Polished
32 – 80 3000, 6000, Fixed or Random h9, h10, h11, k12 Black, Peeled, Turned, Ground, Polished
85 – 150 3000, 6000, Fixed or Random h9, h10, h11, k12 Black, Peeled, Turned, Ground
160 – 300 2000, 3000, Fixed or Random h10, h11, k12 Black, Peeled, Turned, Rough Ground
320 – 500 1000, 2000, Fixed or Random h11, k12 Black, Peeled, Turned
550 – 800 1000, Fixed or Random k12, k13 Black, Rough Turned

Flat Bar Specifications

Thickness (mm) Width (mm) Standard Length (mm) Tolerance Surface Condition
5 – 15 20 – 100 3000, 6000, Fixed or Random EN 10278, EN 10058 Hot Rolled, Cold Drawn, Ground
16 – 30 30 – 150 3000, 6000, Fixed or Random EN 10278, EN 10058 Hot Rolled, Cold Drawn, Ground
32 – 50 40 – 200 3000, 6000, Fixed or Random EN 10058 Hot Rolled, Cold Drawn, Ground
55 – 80 60 – 300 3000, 6000, Fixed or Random EN 10058 Hot Rolled, Cold Drawn
85 – 120 80 – 400 3000, Fixed or Random EN 10058 Hot Rolled
125 – 200 100 – 500 2000, 3000, Fixed or Random EN 10058 Hot Rolled

Plate Specifications

Thickness (mm) Width (mm) Length (mm) Tolerance Surface Condition
5 – 10 Up to 2000 Up to 6000 EN 10029, ASTM A6 Hot Rolled, Pickled, Ground
12 – 25 Up to 2500 Up to 8000 EN 10029, ASTM A6 Hot Rolled, Pickled, Ground
30 – 60 Up to 2500 Up to 10000 EN 10029, ASTM A6 Hot Rolled, Pickled
65 – 100 Up to 2200 Up to 8000 EN 10029, ASTM A6 Hot Rolled
110 – 200 Up to 2000 Up to 6000 EN 10029, ASTM A6 Hot Rolled
220 – 300 Up to 1800 Up to 4000 EN 10029, ASTM A6 Hot Rolled

Square Bar Specifications

Size (mm) Standard Length (mm) Tolerance Surface Condition
10 x 10 – 30 x 30 3000, 6000, Fixed or Random h11, h12, k12 Hot Rolled, Cold Drawn, Ground
35 x 35 – 80 x 80 3000, 6000, Fixed or Random h11, h12, k12 Hot Rolled, Cold Drawn, Ground
85 x 85 – 150 x 150 3000, 6000, Fixed or Random h12, k12 Hot Rolled, Ground
160 x 160 – 300 x 300 2000, 3000, Fixed or Random k12, k13 Hot Rolled

Hexagonal Bar Specifications

Size (mm) Standard Length (mm) Tolerance Surface Condition
10 – 30 (across flats) 3000, 6000, Fixed or Random h11, h12 Hot Rolled, Cold Drawn, Ground
32 – 60 (across flats) 3000, 6000, Fixed or Random h11, h12 Hot Rolled, Cold Drawn, Ground
65 – 100 (across flats) 3000, Fixed or Random h12, k12 Hot Rolled, Cold Drawn

Forged Block Specifications

Thickness (mm) Width (mm) Length (mm) Tolerance Surface Condition
50 – 200 100 – 600 200 – 1000 DIN 7527, ASTM A711 Black, Rough Machined
220 – 400 250 – 800 300 – 1500 DIN 7527, ASTM A711 Black, Rough Machined
420 – 600 350 – 1000 400 – 2000 DIN 7527, ASTM A711 Black, Rough Machined

Forged Round Specifications

Diameter (mm) Length (mm) Tolerance Surface Condition
150 – 300 200 – 1000 DIN 7527, ASTM A711 Black, Rough Machined
320 – 500 300 – 1500 DIN 7527, ASTM A711 Black, Rough Machined
550 – 800 400 – 2000 DIN 7527, ASTM A711 Black, Rough Machined
850 – 1200 500 – 1500 DIN 7527, ASTM A711 Black, Rough Machined

Special Shapes and Custom Dimensions

FUSHUN METAL also offers 41CrAlMo7-10 in custom shapes, sizes, and pre-machined conditions to meet specific application requirements:

  • Near-net shape forgings
  • Pre-machined gear blanks
  • Camshaft and crankshaft blanks
  • Hollow bar and tubes
  • Custom profile sections
  • Semi-finished components
  • Pre-machined tool blanks
  • Custom forged shapes per drawing

Chemical Composition

FUSHUN METAL’s 41CrAlMo7-10 Steel features the following nominal composition per EN 10085 standard:

Element Content (%)
Carbon (C) 0.38-0.45%
Silicon (Si) 0.40% max
Manganese (Mn) 0.40-0.70%
Phosphorus (P) 0.025% max
Sulfur (S) 0.035% max
Chromium (Cr) 1.50-1.80%
Molybdenum (Mo) 0.25-0.35%
Aluminum (Al) 0.70-1.00%
Iron (Fe) Balance

Key Element Functions

  • Carbon (0.38-0.45%): Provides moderate core hardness and strength after heat treatment. The carbon content is optimized to provide good core properties while maintaining excellent nitriding response.
  • Chromium (1.50-1.80%): Enhances hardenability and contributes to the formation of chromium nitrides during nitriding, improving surface hardness and wear resistance.
  • Aluminum (0.70-1.00%): A key alloying element that forms extremely hard aluminum nitrides during the nitriding process, enabling exceptional surface hardness (up to 1100 HV) and nitride case depth.
  • Molybdenum (0.25-0.35%): Improves hardenability, enhances core strength, and helps maintain toughness. Also contributes to high-temperature strength and creep resistance.
  • Manganese (0.40-0.70%): Improves hardenability and contributes to overall strength.
  • Silicon (max 0.40%): Contributes to strength and deoxidation during steelmaking.

Physical and Mechanical Properties

Our 41CrAlMo7-10 Steel offers an impressive combination of physical and mechanical properties that make it ideal for demanding applications:

Physical Properties

Property Units Value
Density g/cm³ 7.85
Melting Range °C 1420-1460
Thermal Conductivity (20°C) W/m·K 42
Specific Heat Capacity J/kg·K 470
Electrical Resistivity Ω·mm²/m 0.22
Modulus of Elasticity (20°C) GPa 210
Coefficient of Thermal Expansion (20-100°C) 10⁻⁶/K 12.5
Coefficient of Thermal Expansion (20-300°C) 10⁻⁶/K 13.5

Mechanical Properties (Quenched and Tempered Condition – Before Nitriding)

Property Value
Core Hardness 28-34 HRC (285-340 HB)
Tensile Strength 950-1150 MPa
Yield Strength 750-900 MPa
Elongation 10-14%
Reduction of Area 40-50%
Impact Strength (Charpy V-notch) 40-60 J

Nitriding Properties

Property Value
Surface Hardness After Gas Nitriding 950-1100 HV0.5
Surface Hardness After Plasma Nitriding 900-1050 HV0.5
Effective Case Depth (550 HV) 0.3-0.7 mm (depending on nitriding time and temperature)
Compound Layer Thickness 10-20 µm (controllable)
Fatigue Strength Improvement 30-50% compared to untreated condition
Wear Resistance Improvement Up to 10 times compared to untreated condition

Applications

FUSHUN METAL’s 41CrAlMo7-10 Nitriding Steel is specifically engineered for applications requiring an optimal combination of high surface hardness, good core strength, and excellent wear resistance:

Automotive Applications

  • Camshafts and camshaft lobes
  • Crankshafts for high-performance engines
  • Transmission gears and shafts
  • Differential gears
  • Steering components
  • Piston pins
  • Valve components
  • Engine timing gears

Industrial Machinery Applications

  • Heavy-duty industrial gears
  • Worm gears and shafts
  • Extrusion screws
  • Spindles and arbors
  • Hydraulic cylinders and rods
  • Drive shafts for high-load applications
  • Pump components
  • Compressor components

Tool and Die Applications

  • Forming dies
  • Cold extrusion tooling
  • Punches and die inserts
  • Gauges and fixtures
  • Plastic molding components
  • Press tooling
  • Forging dies
  • Cutting tools for moderate service

Heavy Equipment Applications

  • Earthmoving equipment components
  • Mining machinery parts
  • Agricultural equipment components
  • Construction machinery parts
  • Gears for heavy equipment
  • Bearing races and rollers
  • High-stress pins and bushings
  • Hydraulic system components

Other Specialized Applications

  • Aircraft landing gear components
  • Turbine and compressor parts
  • Heavy-duty bearing components
  • Railroad equipment parts
  • Marine propulsion system components
  • Oil and gas industry components
  • Defense industry applications
  • Power generation equipment

Heat Treatment Recommendations

For customers performing their own heat treatment of 41CrAlMo7-10 steel, FUSHUN METAL recommends the following parameters:

Stress Relieving

  • Heat slowly to 600-650°C (1110-1200°F)
  • Hold for minimum 2 hours per 25mm of thickness
  • Cool slowly in furnace to below 500°C (930°F), then air cool
  • Recommended before extensive machining to minimize distortion

Normalizing

  • Heat to 880-920°C (1615-1690°F)
  • Hold for 15-30 minutes after thorough heating
  • Cool in still air
  • Resulting hardness: 250-300 HB

Hardening (Pre-Nitriding)

  • Preheat: 550-650°C (1020-1200°F)
  • Austenitizing: 840-880°C (1545-1615°F)
  • Holding time: 15-45 minutes after thorough heating (depending on section size)
  • Quenching: Oil or polymer quench
  • Achievable hardness after quenching: 48-52 HRC

Tempering (Pre-Nitriding)

  • Temper immediately after quenching
  • Tempering temperature: 600-680°C (1110-1255°F) for best nitriding response
  • Holding time: 1-2 hours per 25mm of thickness (minimum 2 hours)
  • Cooling: Air cooling
  • Resulting core hardness: 28-34 HRC (285-340 HB)

Nitriding

  • Pre-cleaning: Thorough cleaning to remove oils, oxides, and contaminants
  • Gas Nitriding:
    • Single-stage process: 490-530°C (915-985°F) for 40-100 hours (depending on required case depth)
    • Two-stage (Floe) process:
      • Stage 1: 500-525°C (930-975°F) with 30-40% dissociation for 5-15 hours
      • Stage 2: 550-565°C (1020-1050°F) with 75-85% dissociation for 5-95 hours (depending on required case depth)
  • Plasma Nitriding:
    • Temperature: 480-530°C (895-985°F)
    • Time: 10-50 hours (depending on required case depth)
    • Gas mixture: N₂:H₂ ratio 1:3 to 3:1 (depending on required layer composition)
  • Salt Bath Nitriding:
    • Temperature: 570-590°C (1060-1095°F)
    • Time: 1-3 hours
  • Achievable surface hardness: 950-1100 HV0.5
  • Typical case depth: 0.3-0.7 mm (depending on process and time)

Post-Nitriding Treatment (Optional)

  • Post-oxidation: 350-400°C (660-750°F) for 20-60 minutes for improved corrosion resistance
  • Fine Lapping or Polishing: Light polishing to improve surface finish after nitriding
  • Low-temperature tempering: 150-200°C (300-390°F) for stress relief after nitriding

Machining Recommendations

To achieve optimal results when machining 41CrAlMo7-10 steel, FUSHUN METAL recommends the following parameters:

Condition: Annealed (200-250 HB)

Operation Tool Material Cutting Speed Feed Rate Depth of Cut Coolant
Turning Cemented Carbide P20-P30 120-150 m/min 0.2-0.4 mm/rev 2-5 mm Yes
Turning High Speed Steel 25-35 m/min 0.1-0.3 mm/rev 1-3 mm Yes
Milling Cemented Carbide P20-P40 100-130 m/min 0.1-0.3 mm/tooth 2-6 mm Yes
Milling High Speed Steel 20-30 m/min 0.05-0.2 mm/tooth 1-4 mm Yes
Drilling High Speed Steel 20-25 m/min 0.05-0.15 mm/rev – Yes
Drilling Cemented Carbide 80-100 m/min 0.1-0.2 mm/rev – Yes
Grinding Silicon Carbide Wheel 25-30 m/sec – 0.005-0.05 mm Yes

Condition: Quenched and Tempered (30-34 HRC)

Operation Tool Material Cutting Speed Feed Rate Depth of Cut Coolant
Turning Cemented Carbide P10-P20 100-130 m/min 0.15-0.3 mm/rev 1-3 mm Yes
Turning High Speed Steel 15-25 m/min 0.1-0.2 mm/rev 0.5-2 mm Yes
Milling Cemented Carbide P10-P30 80-110 m/min 0.1-0.25 mm/tooth 1-4 mm Yes
Milling High Speed Steel 15-22 m/min 0.05-0.15 mm/tooth 0.5-3 mm Yes
Drilling High Speed Steel 15-20 m/min 0.05-0.12 mm/rev – Yes
Drilling Cemented Carbide 60-80 m/min 0.08-0.15 mm/rev – Yes
Grinding Aluminum Oxide Wheel 25-30 m/sec – 0.005-0.03 mm Yes

Post-Nitriding Machining

After nitriding, only grinding, honing, lapping, or superfinishing operations are recommended:

Operation Wheel/Stone Type Speed Feed Depth Coolant
Grinding Aluminum Oxide (Fine) 20-25 m/sec 0.5-1.0 m/min 0.005-0.01 mm Abundant
Honing Diamond or CBN Stone 15-25 m/min – 0.002-0.005 mm Honing Oil
Lapping Cast Iron Lap with Diamond Paste 10-20 m/min – 0.001-0.003 mm Lapping Oil
Superfinishing Fine Abrasive Stone 5-10 m/min – 0.001 mm Light Oil

Welding Recommendations

Welding of 41CrAlMo7-10 is challenging due to its alloying elements but possible with proper precautions:

  • Preheat: 250-350°C (480-660°F)
  • Interpass Temperature: 250-400°C (480-750°F)
  • Post-weld Heat Treatment: Recommended – slow cooling followed by tempering at 600-650°C (1110-1200°F)
  • Filler Materials: Low hydrogen electrodes with similar composition (preferably CrMo type)
  • Processes: TIG/GTAW or MMA/SMAW with low hydrogen electrodes
  • Special Considerations: After welding, the nitriding properties in the weld area will be altered
  • Limitations: For repair purposes only; structural welds not recommended
  • Alternative: Consider mechanical joining methods when possible

Comparative Advantages over Other Similar Grades

Understanding how 41CrAlMo7-10 steel compares to similar grades helps in selecting the optimal material for your application:

Property 41CrAlMo7-10 34CrAlMo5-10 34CrAlNi7-10 31CrMoV9 42CrMo4
Aluminum Content 0.7-1.0% 0.8-1.2% 0.8-1.2% None None
Core Strength Very Good Good Very Good Good Excellent
Nitriding Response Excellent Excellent Excellent Good Moderate
Case Hardness 950-1100 HV 950-1100 HV 950-1100 HV 850-950 HV 700-850 HV
Toughness Very Good Good Excellent Very Good Excellent
Machinability Good Good Good Very Good Very Good
Cost Moderate-High Moderate High Moderate Moderate-Low
Typical Applications Heavy-duty gears, camshafts, highly stressed components Medium-duty gears, shafts, moderate stress parts Aerospace, high-performance components Hot and cold work tools, dies General engineering, non-nitrided applications

Quality Assurance and Testing

Every batch of FUSHUN METAL’s 41CrAlMo7-10 Steel undergoes rigorous testing to ensure it meets our exacting quality standards:

  • Chemical Composition Analysis: Spectrographic testing to verify precise element content critical for performance, with special attention to aluminum, chromium, and carbon levels.
  • Mechanical Property Testing: Tensile testing, hardness testing, and impact testing to verify strength and toughness properties.
  • Microstructural Examination: Metallographic analysis to verify proper structure, grain size, and inclusions.
  • Ultrasonic Testing: 100% ultrasonic inspection for critical applications to ensure internal soundness.
  • Dimensional Inspection: Comprehensive dimensional verification to ensure tight tolerances.
  • Hardenability Testing: Jominy end-quench testing to verify through-hardening capability.
  • Nitriding Response Testing: Sample nitriding tests to verify surface hardness and case depth potential.
  • Cleanliness Testing: Inclusion content analysis to ensure high steel quality.
  • Surface Quality Inspection: Visual and magnetic particle inspection to detect surface defects.
  • Heat Treatment Verification: Testing of heat-treated samples to verify response to thermal processing.

Certifications Provided

  • Material Test Certificates according to EN 10204 3.1
  • Chemical composition analysis
  • Mechanical property test results
  • Dimensional inspection report
  • Heat treatment certification when applicable
  • Special property verifications available upon request
  • Certificate of conformity to ordered specifications
  • Ultrasonic testing reports when specified
  • Nitriding response test reports when specified

Why Choose FUSHUN METAL for 41CrAlMo7-10 Steel

When you select FUSHUN METAL as your supplier for 41CrAlMo7-10 Steel, you partner with a leading manufacturer committed to excellence:

  • Comprehensive Product Range: Extensive range of product forms to meet diverse application requirements.
  • Technical Expertise: In-depth knowledge of nitriding steels and their applications.
  • Custom Solutions: Ability to provide custom shapes, sizes, and pre-processed components.
  • Quality Assurance: Stringent quality control processes ensuring consistent properties.
  • Metallurgical Support: Technical guidance for material selection, heat treatment, and application optimization.
  • Global Supply Capability: Reliable worldwide shipping and logistics solutions.
  • Cost-Effective Solutions: Competitive pricing combined with superior quality and service.
  • Industry Experience: Extensive experience serving automotive, aerospace, and industrial machinery sectors.
  • Innovation: Ongoing research and development to enhance product performance.
  • Sustainability Focus: Commitment to environmentally responsible manufacturing practices.
  • Rapid Delivery: Extensive inventory of standard sizes for quick delivery.
  • Complete Documentation: Comprehensive certification and testing reports.

Request Information

Contact FUSHUN METAL today to discuss your 41CrAlMo7-10 Steel requirements. Our technical team is ready to assist you with:

  • Detailed product specifications
  • Technical consultations for your specific application
  • Heat treatment recommendations for optimal properties
  • Custom dimension and processing requirements
  • Pricing inquiries and delivery schedules
  • Sample requests for evaluation

FUSHUN METAL – Your trusted partner for premium nitriding steel solutions that deliver consistent quality, superior surface hardness, and excellent core strength for the most demanding industrial applications.

 

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x