XM-32, S6412, Stainless Steel For Turbine Blades

XM-32, S6412, Stainless Steel For Turbine Blades

WHY CHOOSE US

In addition to providing the widest range of materials to many different sectors, we are the only company who can melt and forge according to customer requests and produce in the form closest to the final product. We provide services that will increase the added value in products by adding our mechanical processing and heat treatment capabilities to our forging products, which are produced in requested forms from automotive to energy, from maritime to mold industry.

 

SPECIFICATIONS               

AIR : Z 12 CNDV 12

WL : 1.4933

BS : S 151, S 538, S 159

UNS : S64152

WL : 1.4939

UNS : S64152

AMS : 5719

 

APPLICATIONS

  • Aerospace industry: various mechanical parts.
  • Turbine blades and discs.

 

CHARACTERISTICS

  • Good resistance to various corrosive agents.
  • Good weldability and suitable for brazing

 

CHEMICAL COMPONENT

Grade UNS Carbon Manganese Phosphorus Sulfur Silicon Chromium Nickel Molybdenum Vanadium Nitrogen
XM-32 S64152 0.08–0.15 0.50–0.90 0.025 0.025 0.35max 11.00–12.50 2.00–3.00 1.50–2.00 0.25–0.40 0.01–0.05

 

 

MECHANICAL PROPERTIES

  • Annealed condition: heat to 680°C followed by slow cooling.

– Brinell Hardness: 255

 

  • Air cool from 1050°C. Temper at 250°C.

– UTS:1350 N/mm2

– 0.2 % Yield strength:1000 N/mm2

– Elongation (5d): 17 %

– Impact strength KCU:110 J/cm2

 

  • Air cool from 1050°C. Temper at 650°C.

– UTS:1050 N/mm2

– 0.2 % Yield strength:700 N/mm2

– Elongation (5d):15 %

– Impact strength KCU:120 J/cm2

 

  • Creep:
TemperatureIn ℃ Average load in N/mm²

causing creep
fracture in:

Average load in N/mm²

causing 1%

elongation in:

100 hrs 1000 hrs 100 hrs 1000 hrs
500 500 420 430 370

 

 

HEAT TREATMENT

Hardening:

Heat to 1050°C Air cool or oil quench.

 

Temper:

Depending on properties required.

 

PHYSICAL PROPERTIES

  • Density:8
  • Thermal conductivity in W.m/m2°C:- at 20°C: 21
  • Mean coefficient of expansion in m/m.°C:
  • -between 20°C and 100°C:9.7 x 106
  • -between 20°C and 300°C:10.4 x 10-6
  • -between 20°C and 500°C:11.2 x 106
  • Modulus of elasticity in N/mm2 – at 20°C:211 x 103

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x