Alloy 4130 (AISI 4130) is a chromium molybdenum alloy steel being a widely used Aircraft Steel due to its weldability, ease of fabrication and mild hardenability. The hardenability and weldability of Alloy 4130 are considered equivalent to 8630 (MIL-S-6250) . Alloy 4130 is also vacuum degassed to meet the magnetic particle inspection standards of AMS 2301.

<<AMS MIL 4130 DATA SHEET>>

 

Aircraft Quality 4130 per 6345 & 6350 Cold Rolled Sheet

Chromaloy Steel 4130 (E4130) combines Chromium and Molybdenum to maximize strength in this heat-treatable Aircraft Quality AISI 4130 alloy steel. The term Aircraft Quality (or AQ Steel) which is common to all steel at Benedict-Miller means it is suitable for the production of aircraft parts which are subject to magnetic particle inspection after machining.

 

Specifications

AMS 6345 Sheet / Plate, Normalised

AMS 6346 Bar Hardened & Tempered

AMS 6350 Sheet / Plate

AMS 6351 Sheet / Plate, spheroidised

AMS 6370 Bar

AMS 6371 Tube

MIL-S-6758

MIL-S-18729

MIL-T-67366

AISI 4130

 

Applications of 4130 Chrome- Moly Aircraft Steel :

Automotive

Military / Commercial Aircraft

Machine Tools

Components

Motorsports

Aerospace

Oil and Gas industry

 

Chemical Composition Limits

Weight% C Mn P S Si Cr Ni Mo Cu
4130 Bar/Tube 0.28 – 0.33 0.40-0.60 0.025 max 0.025 max 0.15 – 0.35 0.80-1.10 0.25 max 0.15-0.25 0.35
4130 Sheet/Plate 0.28 – 0.33 0.40 – 0.60 0.025 max 0.025 max 0.20-0.35 0.80-1.10 0.15 – 0.25

 

Typical Mechanical Properties

Alloy Condition Thickness Tensile Strength ksi Yield Strength ksi Elongation Hardness
Tube AMS 6371 Cold Drawn 95 70 12 <25
Bar AMS 6370 Annealed 29HB Max
Bar AMS 6346 Hardened & Tempered 125 100 17
Sheet AMS 6350 Annealed <25 HRC
Sheet AMS 6345 Normalised <0.062″ 95 75 8
Sheet AMS 6345 Normalised 0.062″ – 0.125″ 95 75 10
Sheet AMS 6345 Normalised 0.125″ – 0.187″ 95 75 12
Sheet AMS 6345 Normalised 0.187″ – 0.250″ 90 70 15
Sheet AMS 6345 Normalised 0.250″ – 0.750″ 90 70 16
Sheet AMS 6345 Normalised 0.750″ – 1.500″ 90 70 18
Sheet AMS 6345 Normalised & Heat Treated 0.249″ – 0.375″ 42
Sheet AMS 6345 Normalised & Heat Treated 0.375″ – 0.500″ 38
Sheet AMS 6345 Normalised & Heat Treated 0.500″ – 0.625″ 32
Sheet AMS 6345 Normalised & Heat Treated 0.625″ – 0.750″ 29
Sheet AMS 6345 Normalised & Heat Treated 0.750″ – 0.875″ 27
Sheet AMS 6345 Normalised & Heat Treated 0.875″ – 1.500″ 26

 

We also supply
MARS190 D6AC AMS 4130
AMS 4340 MOD AMS 4340 AMS 4330 MOD
AMS 9310 AMS 13-8 PH AMS 15-5 PH
AMS 17-4 PH AMS 625 AMS 718
AerMet® 100 Maraging 250 Maraging 300
Maraging 350 Titanium Grade 5 Ti-6Al-4V ELI Titanium

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x