1.2394 Tool Steel
Cold work tool steels
<<1.2394 Tool Steel DATA SHEET>>
Cutting:
Precision cutting to standard dimensions
Custom cutting according to client specifications
Cold Work Tool Steel Dimensions
We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.
| Product Form | Specifications |
|---|---|
| Forged Round Bar | Dia. up to 1200mm |
| Forged Flat Bar | Thickness 100-600mm, Width 300-2000mm |
| Rolled Round Bar | Dia. 10-200mm |
| Hot Rolled Plate | Thickness 1-100mm, Width 60-1600mm |
Designation by Standards
| Brand Name | LH No. | Mat. No. |
| OH252 | 252 | 1.2394 |
Chemical Composition (in weight %)
| C | Si | Mn | Cr | Mo | V |
| 0.50 | 0.90 | 0.80 | 7.90 | 1.50 | 1.70 |
Description
Medium alloyed cold work steel tool steel with high toughness and wear resistance.
Applications
Severely stressed machine blades for cellulose and paper industry, woodworking milling cutters, flat and circular blades for cutting sheets/plates of thickness 5 to 15 mm.
Physical properties (average values) at ambient temperature
Module of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.80
Hardening
Harden from a temperature of 1080-1120℃ followed by oil quenching.
Forging
Hot forming temperature: 1100-900℃.