310moln stainless steel grade is a fully austenitic stainless steel that does not have intermetallic phases such as intergranular carbide precipitations. For applications in urea plants 310MoLN steel grade has a specifically designed optimized chemical composition. To stabilize and strengthen the austenitic phase the nitrogen in the chemical composition helps. 310 MoLN, material gives excellent corrosion-resistance in urea carbamate environments such as high-pressure strippers.  Among wrought austenitic stainless steels it has a fairly high base cost. And it has a fairly high embodied energy and a fairly low ductility.

 

<<310MoLN, 1.4466, Stainless Steel DATA SHEET>>

 

Material

Material designation
1.4466 SEL
S31050 UNS
X1CrNiMoN25-22-2 EN
310 MOLN AISI
Standards
10088-3 EN ISO
310MoLn A182 ASTM

 

Chemical Composition

SS 310MoLN WNR

1.4466

UNS

S31050

AISI

310MoLN

GRADE

310MoLN

AFNORZ1C ND25.22AZ
Carbon 0.020max 0.020max 0.020max 0.020max 0.020max 0.020max
Manganese 2.00max 2.00max 2.00max 2.00max 2.00max 2.00max
Chromium 24.0-26.0 24.0-26.0 24.0-26.0 24.0-26.0 24.0-26.0 24.0-26.0
Phosphorus 0.025max 0.025max 0.025max 0.025max 0.025max 0.025max
Sulfur 0.010max 0.010max 0.010max 0.010max 0.010max 0.010max
Molybdenum 2-2.50 2-2.50 2-2.50 2-2.50 2-2.50 2-2.50
Nickel 21.0-23.0 21.0-23.0 21.0-23.0 21.0-23.0 21.0-23.0 21.0-23.0
Nitrogen 0.10-0.16 0.10-0.16 0.10-0.16 0.10-0.16 0.10-0.16 0.10-0.16
Silicon 0.70max 0.70max 0.70max 0.70max 0.70max 0.70max
Iron Bal Bal Bal Bal Bal Bal

 

Mechanical Properties

SS 310MoLN WNR

1.4466

UNS

S31050

AISI

310MoLN

GRADE

310MoLN

AFNORZ1 CND25.22AZ
Tensile Strength,

Mpa(psi)

540-740

(78320-107327)

540-740

(78320-107327)

540-740

(78320-107327)

540-740

(78320-107327)

540-740

(78320-107327)

540-740

(78320-107327)

Yield Strength,

Mpa(psi)

250(36259) 250(36259) 250(36259) 250(36259) 250(36259) 250(36259)
Elongation % 40 40 40 40 40 40
Reduction in Area, %
Hardness, Brinell 95 95 95 95 95 95

 

The grade is characterized by :

  • Excellent resistance to corrosion in ammonium carbamate and nitric acid
  • Excellent resistance to intergranular corrosion
  • High resistance to pitting and crevice corrosion
  • Good weldability

Applications:

  • Striper Tubes
  • Outerlayer of bimetallic
  • Ferrules
  • Carbamate Condensers
  • Decomposers
  • Reactor Coils

General corrosion

  • S31050 was originally developed for stripper tubes used in the production of urea.
  • S31050 has excellent corrosion resistance in urea/carbamate solutions at high pressures andtemperatures.
  • S31050 is also highly resistant to inorganic acids

Intergranular corrosion

  • S31050 ishighly resistant to intergranular corrosion after welding.

Pitting and crevice corrosion

  • S31050 has very good resistance to pitting, and is also far more resistant to crevice corrosion than ASTM 316L.

Stress corrosion cracking (SCC)

  • Conventionalausteniticstainless steels of type ASTM 304 and 316 are susceptible to stress corrosion cracking (SCC) in chloride- bearing solutions at temperatures exceeding about 60°C (140°F). The higher nickel content makes S31050 slightly more resistant

Erosion corrosion

  • The good mechanical strength of S31050 makes it resistant to erosion-corrosion. Ferrules for urea strippers are oneapplicationwhere this property is utilised.

Weldability

  • Theweldability of S31050 is good. Welding must be carried out without preheating, and normally there is noneed for any subsequent heat treatment.
  • S31050 has lowthermal conductivity and high thermal expansion.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x