manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

20meters Length Hardened Turned Steel Bar And Shaft

20meters Length Hardened Turned Steel Bar And Shaft

Super Duplex F55 S32760 Stainless Steel

We offer hardened and turned steel bars and shafts up to 20 meters in length, suitable for a variety of mechanical and industrial applications. These products include carbon steel, alloy steel, and special steel, processed with centerless turning and centerless grinding to ensure high precision and excellent surface quality. We also provide chrome plating and borehole services for hydraulic systems, meeting various specialized requirements.

 

Materials:

We offer a diverse range of materials to cater to various industrial and mechanical applications, ensuring that our steel bars and shafts meet the highest standards of quality and performance.

– 4130: A versatile chromium-molybdenum alloy steel, 4130 offers good strength, weldability, and toughness. It is frequently used in aircraft structures, racing car frames, and other applications requiring a combination of strength and light weight.

 

– 4140:  With higher carbon content than 4130, 4140 alloy steel delivers increased strength and hardness. It is commonly used for gears, shafts, spindles, and other heavy-duty machinery components that need to withstand high stress and wear.

 

– 4150:  Containing even more carbon than 4140, 4150 alloy steel provides exceptional strength and hardness. It is well-suited for high-performance applications like gears, shafts, and other heavily loaded components where wear resistance is crucial.

 

– 4137: A modification of 4130, 4137 alloy steel has a slightly lower carbon content. This makes it easier to machine and weld while still maintaining good strength and toughness. It is often used for similar applications as 4130, but where enhanced machinability is desired.

 

– 4330V:  Also known as 300M, 4330V is a vacuum-melted alloy steel with exceptional strength, toughness, and fatigue resistance. It is used in demanding applications like aerospace components, high-performance gears, and racing car parts.

 

– 4340:  Similar to 4140, 4340 alloy steel has the addition of nickel, which further enhances its hardenability and toughness. It is widely used for heavy-duty gears, shafts, and other components requiring high strength and impact resistance.

 

– 4145H:  The “H” designation indicates that 4145H alloy steel has been specifically processed to achieve a higher hardenability. This makes it suitable for applications requiring a hard, wear-resistant surface, such as gears, shafts, and other machine parts.

 

– 5120: An alloy steel with good case hardening properties, 5120 is typically used for gears, shafts, and other components that require a hard surface and a tough core.

– 5140: Known for its good balance of toughness, strength, and wear resistance, 5140 alloy steel is often used in the automotive and machinery industries for making axles, shafts, and gears.

– SCM420: This low-alloy steel offers excellent hardenability and strength, making it suitable for a variety of high-stress applications such as gears and crankshafts.

– SCr440: With higher carbon content, SCr440 provides superior wear resistance and strength, commonly used in the production of high-performance gears and mechanical parts.

– 20Cr4: A low-alloy steel with good hardenability, 20Cr4 is widely used for components that require high tensile strength and toughness, such as transmission parts and machine shafts.

– 41Cr4: Known for its excellent hardenability and mechanical properties, 41Cr4 is often used in the automotive and engineering industries for making parts like gears, axles, and crankshafts.

 

Our selection of carbon and alloy steels ensures that we can provide the optimal material for your specific needs, delivering products that offer superior performance, durability, and reliability in demanding industrial applications.

 

Size:

We understand that precision and suitability are crucial for industrial applications, which is why we offer steel bars and shafts in a variety of sizes to meet diverse requirements. Our products are manufactured to precise specifications to ensure optimal performance in their intended applications.

Diameter:

Our steel bars and shafts are available in a wide range of diameters, from 30 mm to 200 mm. This range allows us to cater to various needs, whether it’s for small, intricate components or larger, more robust parts. The extensive diameter options ensure that you can find the perfect size for your specific project, enhancing the efficiency and functionality of your machinery.

Length:

We provide steel bars and shafts in lengths up to a maximum of 20 meters. This significant length capacity is ideal for applications requiring long, continuous pieces of material, such as in construction, manufacturing, and heavy machinery industries. The ability to supply such long lengths reduces the need for additional welding or joining, thus maintaining the structural integrity and strength of the material.

 

Our commitment to offering a broad size range ensures that you can source the exact dimensions needed for your projects, reducing waste and improving overall productivity. Whether you require standard or custom sizes, our wide selection of diameters and lengths ensures that we can meet your specific requirements with precision and reliability.

1.4006 X12Cr13 Martensitic Stainless Steel

Surface:

We place a high emphasis on surface quality, as it plays a critical role in the performance and longevity of steel bars and shafts in various applications. To meet diverse needs and ensure the highest level of precision and smoothness, we offer several surface treatments:

Peeled:

Peeled surfaces involve the removal of the outer layer of the material to eliminate any imperfections such as scales, decarburization, or minor surface defects. This process produces a smooth, clean finish that enhances the material’s appearance and prepares it for further processing. Peeled steel bars and shafts are ideal for applications requiring a high degree of dimensional accuracy and surface integrity.

Polished:

Polished surfaces undergo a series of abrasive processes to achieve a highly smooth and reflective finish. This treatment not only improves the aesthetic appeal but also enhances the material’s resistance to corrosion and wear. Polished steel bars and shafts are commonly used in applications where a superior surface finish is critical, such as in the manufacturing of precision instruments, medical devices, and high-end machinery components.

Turned:

Turned bright surfaces are achieved through precision turning operations that produce a bright, shiny finish with excellent dimensional accuracy. This process removes surface irregularities and provides a uniform, visually appealing appearance. Turned bright steel bars and shafts are particularly suited for applications that demand both high mechanical performance and an attractive finish, including automotive parts, hydraulic systems, and general engineering components.

 

By offering these advanced surface treatments, we ensure that our steel bars and shafts not only meet but exceed the stringent requirements of various industrial applications. Each treatment option is designed to enhance the material’s functionality, durability, and overall performance, making our products the ideal choice for a wide range of demanding environments.

 

Condition:

To ensure our steel bars and shafts deliver optimal performance and durability, we provide them in a specific heat-treated condition known as quenched and tempered. This treatment process significantly enhances the mechanical properties of the steel, making it suitable for a wide range of demanding applications.

Quenched:

Quenching is a meticulous heat treatment process where the steel is heated to a high temperature and then rapidly cooled in water, oil, or another cooling medium. This rapid cooling transforms the microstructure of the steel, increasing its hardness and strength. Quenching helps in achieving the desired mechanical properties, particularly in applications that require high wear resistance and the ability to withstand heavy loads. The process reduces internal stresses and prepares the steel for further tempering to refine its properties.

Tempered:

After quenching, the steel undergoes tempering, a controlled reheating process to a temperature below its critical point, followed by cooling at a slower rate. This step is crucial as it reduces the brittleness induced by quenching and enhances the toughness and ductility of the steel. Tempering allows for the fine-tuning of mechanical properties, striking a balance between hardness and toughness, which is essential for components subjected to dynamic loads and varying operational conditions. The tempering process also improves the steel’s overall stability and resistance to cracking under stress.

 

By providing our steel bars and shafts in a quenched and tempered condition, we ensure that they possess a superior combination of strength, hardness, and toughness. This makes them ideal for high-performance applications such as automotive components, heavy machinery, construction equipment, and critical engineering parts. Our meticulous heat treatment processes guarantee that the materials can withstand extreme conditions and deliver reliable, long-lasting performance in the most demanding industrial environments.

HS3-3-2, 1.3333, High-speed Tool Steel

More Services:

In addition to offering high-quality steel bars and shafts, we provide a range of specialized services to enhance the functionality and performance of our products. These additional services are designed to meet specific requirements and improve the overall utility of the materials in various applications.

Chromed:

Our chroming service involves applying a layer of chromium to the surface of the steel bars and shafts through an electroplating process. This treatment provides several key benefits:

– Corrosion Resistance: The chromium layer acts as a protective barrier against oxidation and corrosion, significantly extending the lifespan of the steel in harsh environments.

– Wear Resistance: Chrome plating increases the surface hardness, making the steel more resistant to wear and abrasion, which is critical for components that experience high friction and mechanical stress.

– Aesthetic Appeal: The bright, reflective finish of chrome plating enhances the visual appeal of the steel, making it suitable for applications where appearance matters.

Chromed steel bars and shafts are ideal for use in hydraulic cylinders, automotive parts, and machinery components that require both durability and a high-quality finish.

Borehole:

Our borehole service involves precision drilling of holes into the steel bars and shafts according to specific requirements. This service is essential for creating internal passages and cavities that are critical for various applications:

– Hydraulic Systems: Boreholes allow for the integration of fluid channels in hydraulic cylinders and actuators, facilitating the efficient flow and control of hydraulic fluids.

– Custom Components: Boreholes enable the creation of custom parts with specific internal features, such as hollow shafts, which reduce weight without compromising strength.

– Enhanced Functionality: By providing precisely machined boreholes, we ensure that the steel components meet exact specifications, enhancing their functionality and performance in complex assemblies.

Our borehole service is performed using advanced machining techniques to ensure high precision and consistency, catering to the diverse needs of industries such as automotive, aerospace, and heavy machinery.

 

These additional services underscore our commitment to delivering comprehensive solutions that meet the exacting standards of our customers. By offering chroming and borehole services, we add value to our steel bars and shafts, ensuring they are equipped to excel in their intended applications.

 

Application:

Our high-quality steel bars and shafts are designed to serve a broad spectrum of industrial applications, ensuring reliability, durability, and superior performance across various sectors. Here are some of the primary applications where our products excel:

Core Rod for Pipe Rolling Process:

In the pipe rolling process, precision and strength are paramount. Our steel bars and shafts are ideally suited as core rods, playing a critical role in the manufacture of seamless pipes and tubes.

– Durability: The high-strength and wear-resistant properties of our steel ensure that the core rods can withstand the intense pressures and temperatures involved in the rolling process.

– Precision: The dimensional accuracy and smooth surface finish of our steel products contribute to the production of high-quality pipes with consistent wall thickness and superior structural integrity.

– Versatility: Suitable for various types of rolling processes, including hot rolling and cold rolling, our core rods are indispensable in industries such as oil and gas, construction, and automotive manufacturing.

Hydraulic System:

Hydraulic systems require components that can endure high pressures and operate seamlessly over long periods. Our steel bars and shafts are engineered to meet these demanding requirements, making them an excellent choice for hydraulic applications.

– Strength and Toughness: The quenched and tempered condition of our steel provides the necessary strength and toughness to handle the high pressures encountered in hydraulic systems.

– Corrosion Resistance: With additional services like chrome plating, our steel components offer enhanced resistance to corrosion, ensuring longevity and reliability even in harsh environments.

– Precision Machining: Our borehole services enable the creation of precise internal passages and cavities, crucial for the efficient flow of hydraulic fluids in cylinders, actuators, and pumps.

– Wide Application: From construction machinery and industrial equipment to automotive systems and aerospace technologies, our steel bars and shafts are integral to the performance and reliability of hydraulic systems across various industries.

ASTM B637 UNS N07718 W.Nr.2.4668 API 6A 718 Inconel 718 Heat Resistant Alloys

By leveraging our expertise in material science and precision engineering, we ensure that our steel bars and shafts meet the stringent requirements of these critical applications. Whether used as core rods in pipe rolling or as vital components in hydraulic systems, our products deliver unmatched performance and reliability, contributing to the success of our customers’ operations.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.