manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

High Speed Steel Plate & Sheet For Sawing Tools

High Speed Steel Plate & Sheet For Sawing Tools

High Speed Steel Plate & Sheet For Sawing Tools

High Speed Steel Plate & Sheet For Sawing Tools

FUSHUN SPECIAL STEEL is proud to present our premium line of High Speed Steel (HSS) plates and sheets, specifically engineered for the production of high-quality sawing tools.

 

At FUSHUN SPECIAL STEEL, we understand the critical role that material quality plays in the performance of sawing tools. Our HSS plates and sheets are manufactured using advanced metallurgical processes to ensure optimal microstructure and properties. This results in tools that maintain their sharp edge longer, resist wear better, and provide superior cutting performance in demanding applications.

 

Applications:

Our high-speed steel plates and sheets are ideal for manufacturing:

Knife tools

Cutting tools

Automotive accessories

Wear-resistant components

Automation industry parts

 

Capacity Range & Tolerance:

Thickness: 0.9-5.0mm

Width: 6-30mm

Thickness Tolerance: ±0.02mm to ±0.05mm (depending on thickness)

Width Tolerance: ±0.03mm to ±0.05mm (depending on width)

Decarburization: ≤0.03mm (≤0.1mm for thicker sheets)

 

Grade Equivalent

GB AISI DIN JIS
W6Mo5Cr4V2 M2 1.3343 SKH51
CW6Mo5Cr4V3 M3 Class SKH53
M4 M4 TSP4
W6Mo5Cr4V2Co5 M35 S6525 SKH55
W2Mo9Cr4VCo8 M42 1.3247 SKH55
W18Cr4V M0 HS18-0-1 SK0
Cr12MoV D2 1.2601 SKD11
Cr12Mo1V1 D2 1.2601 SKD11
95Cr18 A276-440C SUS440C
11Cr17 SUS440C

 

Chemical Component

Grade C Si Mn P≤ S≤ Cr Mo V W Co Cu Ni
M2 0.80-0.90 0.20-0.45 0.15-0.40 ≤0.030 ≤0.030 3.80-4.40 4.50-5.50 1.75-2.20 5.50-6.75 ≤0.25 ≤0.30
M3 Class 1.25-1.32 ≤0.70 0.15-0.40 ≤0.030 ≤0.030 3.75-4.50 4.70-5.20 2.70-3.20 5.90-6.70
M4 1.25-1.40 0.20-0.45 0.15-0.40 ≤0.030 ≤0.030 3.75-4.50 4.50-5.50 3.75-4.50 5.25-6.50
M35 0.87-0.95 0.20-0.45 0.15-0.40 ≤0.030 ≤0.030 3.80-4.50 4.70-5.20 1.70-2.10 5.90-6.70 4.50-5.00
M42 1.05-1.15 0.15-0.65 0.15-0.40 ≤0.030 ≤0.030 3.50-4.25 9.0- 10.0 0.95-1.35 1.15- 1.85 7.75-8.75
M0 0.73-0.83 0.20-0.40 0.10-0.40 ≤0.030 ≤0.030 3.80-4.50 1.0-1.20 17.2-18.7
D2 1.45-1.70 ≤0.40 ≤0.40 ≤0.030 ≤0.030 11.00-12.50 0.40-0.60 0.15-0.30 ≤0.25 ≤0.30
D2 1.40-1.60 ≤0.60 ≤0.60 ≤0.030 ≤0.030 11.00-13.00 0.70-1.20 0.50~ 1.10 ≤0.60 ≤0.25 ≤0.30
A276-440C 0.90-1.00 ≤0.80 ≤0.80 ≤0.040 ≤0.030 17.00-19.00 ≤0.60
SUS440C 0.95-1.20 ≤1.00 ≤1.00 ≤0.040 ≤0.030 16.00-18.00 ≤0.75 ≤0.60

 

Whether you’re producing industrial saw blades, precision cutting tools, or specialized components for the automotive or automation sectors, our high-speed steel plates and sheets offer the perfect balance of hardness, toughness, and machinability.

 

Contact FUSHUN SPECIAL STEEL today to discuss how our high-speed steel plates and sheets can elevate the quality and performance of your sawing tools and other precision components. Let us be your partner in achieving excellence in cutting-edge technology.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x