manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Tool Steel For Cutter Blade

Tool Steel For Cutter Blade

Tool Steel For Cutter Blade

Tool Steel For Cutter Blade

FUSHUN SPECIAL STEEL is a comprehensive professional manufacturing enterprise integrating smelting, electroslag remelting, forging, rolling, heat treatment, and mechanical processing.

 

The company specializes in producing various high-speed tool steels, cold work die steels, hot work die steels, and various special steels. In addition, the company also has complete production lines for high-speed steel circular saw blades, woodworking planer blades, and other cutting tools.

 

Shapes

Wires & Rod

Round Bar

Flat Bar

Plate & Sheet

Strips

 

Grade Equivalent

GB JIS ASTM DIN
Cr12Mo1V1   D2 1.2379
Cr12MoV SKD11   1.2601
5Cr8MoVSi   A8B 1.236
4Cr5MoSiV1 SKD61 H13 1.2344
Cr8Mo1VSi MOD FIED DC11 DC53  
9Cr18Mo SUS440C 440C  
Cr12 SKD1 D3 1.208
9CrWMn SKD3 O1 1.251
    LD  
CrWMn      
W18Cr4V SKH2 T1 1.3355
W6Mo5Cr4V2 SKH51 M2 1.3343
W6Mo5Cr4V2Co5 SKH55 M35 1.3243
W6Mo5Cr4V2Co2      
W5      
W4Mo3Cr4VSi   4341  

 

Chemical Component

Grade C Si Mn P S Cr Mo W V Co
D2 1.45-1.60 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 11.0-12.5 0.7-1.2   0.7-1.0  
1.2601 1.45-1.60 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 11.0-12.5 0.4-0.6   0.15-0.36  
A8B 0.55-0.65 0.9-1.2 0.2-0.4 ≤0.030 ≤0.030 7.5-8.5 1.3-1.6 0.7-1.0 0.3-0.6  
H13 0.32-0.45 0.8-1.2 0.2-0.4 ≤0.030 ≤0.030 1.75-5.5 1.1-1.75 – 0.8-1.2  
DC53 0.9-1.05 0.8-1.1 0.2-0.4 ≤0.030 ≤0.030 7.8-8.5 1.8-2.1   0.15-0.35  
440C 0.95-1.1 ≤0.80 ≤0.80 ≤0.030 ≤0.030 17.0-19.0 0.2-0.75   0.1-0.2  
D3 2.0-2.3 ≤0.40 ≤0.40 ≤0.030 ≤0.030 11.5-13.0        
O1 0.85-0.95 ≤0.40 0.9-1.2 ≤0.030 ≤0.030 0.5-0.8 – 0.5-0.8    
LD 0.65-0.75 0.7-1.2 ≤0.50 ≤0.030 ≤0.030 6.5-7.5 2.0-2.5   1.7-2.2  
CrWMn 0.9-1.05 ≤0.40 0.8-1.1 ≤0.030 ≤0.030 0.9-1.2   1.2-1.6    
T1 0.7-0.8 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4   17.5-19.0 1.0-1.4  
M2 0.8-0.9 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4 4.6-5.0 5.6-6.5 1.75-2.25  
M35 0.85-0.95 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4 4.6-5.0 5.6-6.5 1.75-2.25 4.6-5.0
W6Mo5Cr4V2Co2 0.9-1.0 0.2-0.4 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4 4.6-5.0 5.6-6.0 1.75-2.25 1.8-2.2
W5 0.9-1.0 0.8-1.2 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4 1.6-2.0 4.6-5.0 0.8-1.2  
4341 0.9-1.0 0.8-1.2 0.2-0.4 ≤0.030 ≤0.030 3.8-4.4 2.6-3.0 3.5-4.5 1.2-1.4  

 

FUSHUN SPECIAL STEEL has always adhered to the business philosophy of quality first and credibility above all. We wish to establish long-term friendly cooperative relationships with domestic and overseas customers! If you have any needs for our products, please feel free to contact us. FUSHUN SPECIAL STEEL will provide the best prices and hopes to become your reliable partner.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.