Fushun are main manufacturer of tool steel for Trimming Mould.

 

What is Trimming Mould?

Trimming moulds are precision tools designed for removing excess material or flash from formed parts, particularly after forging, stamping, or casting operations. These moulds consist of carefully engineered cutting edges, support structures, and guiding systems that work together to achieve clean, precise cuts along predetermined trim lines. The design emphasizes accurate alignment and proper clearances to ensure consistent cutting quality.

 

The main function of trimming moulds is to achieve final part dimensions by removing unwanted material from workpieces. They are extensively used in automotive, aerospace, and general manufacturing industries to finish parts like forgings, castings, and pressed components. Trimming moulds can handle various material thicknesses and shapes, operating at high production rates while maintaining precise cut quality and dimensional accuracy. This process is crucial for preparing parts for subsequent operations or final assembly.

 

The materials used in trimming moulds require specific alloying elements to provide optimal performance under repeated impact and shearing forces. These tool steels typically contain high percentages of chromium (8-12%), tungsten (2-6%), and molybdenum (1-3%) to achieve the necessary hardness and wear resistance. The material composition enables hardness levels of 58-62 HRC while maintaining adequate toughness to prevent chipping. The microstructure features uniformly distributed carbides that provide excellent wear resistance and edge retention. Special heat treatments and surface modifications are often applied to enhance durability and reduce maintenance requirements.

Trimming Mould Materials

1.2824 70MnMoCr8 7CrMn2Mo
  — Cr8Mo2SiV
  — 8Cr3

 

Chemical Composition of Trimming Mould

Grade C Si Mn Cr Mo V
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20 0.90~1.40  
Cr8Mo2SiV C.95~1.03 0.80~1.20 0.20~0.50 7.80~8.30 2.00~2.80 0.25~0.40
8Cr3 0.75~0.85 ≤0.40 ≤0.40 3.20~3.80     

 

Properties of Trimming Mould Steel

 

Grade Annealed HBW Hardened HRC
7CrMn2Mo ≤235 61
Cr8Mo2SiV ≤255 62
8Cr3 207~255  

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x