Fushun are main manufacturer of tool steel for Hot Stamping Mould.

 

What is Hot Stamping Mould?

Hot stamping moulds (or Hot punching moulds) are specialized tooling systems designed for forming and punching metal components at elevated temperatures. These moulds incorporate sophisticated heating and cooling systems, precise punching elements, and thermal management features. The mould assembly must maintain dimensional accuracy while handling both high temperatures and significant punching forces, typically including integrated temperature control channels and specialized thermal insulation zones.

 

The primary function of hot stamping moulds is to produce high-strength components through combined heating, forming, and rapid cooling processes. They are extensively used in automotive and aerospace industries to manufacture structural components requiring high strength and precise geometry. This process is particularly effective for ultra-high-strength steel components, offering advantages such as reduced springback, improved formability at elevated temperatures, and enhanced final mechanical properties. The process can achieve complex geometries while ensuring consistent part quality and superior strength characteristics.

 

The mould materials used in hot stamping applications contain specific alloying elements to withstand both thermal and mechanical stresses. Premium grade tool steels are employed, incorporating combinations of chromium, tungsten, molybdenum, and vanadium to provide optimal performance at elevated temperatures. These materials offer excellent hot hardness, thermal fatigue resistance, and wear resistance under high-temperature conditions. The microstructure features thermally stable carbides that maintain hardness and dimensional stability during repeated thermal cycles. Advanced surface treatments and coatings are often applied to enhance wear resistance and thermal shock resistance, while sophisticated cooling systems help maintain precise temperature control during the stamping process.

Hot Stamping Mould Materials

—   8Cr3
H10 1.2365 4Cr3Mo3SiV
—   3Cr3Mo3W2V

 

Chemical Composition of Hot Stamping Mould

Grade C Si Mn Cr W Mo V
8Cr3 0.75~0.85 ≤0.40 ≤0.40 3.20~3.80       
4Cr3Mo3SiV 0.35~0.45 0.80~1.20 0.25~0.70 3.00~3.75   2.00~3.00 0.25~0.75
3Cr3Mo3W2V 0.32~0.42 0.60~0.90 ≤0.65 2.80~3.30 1.20~1.80 2.50~3.00 0.80~1.20

 

Properties of Hot Stamping Mould Steel

 

Grade Annealed HBW
8Cr3 207~255
4Cr3Mo3SiV ≤229
3Cr3Mo3W2V ≤255

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x