Hot Forging Mould Tool Steel

Hot Forging Mould Tool Steel

Hot Forging Mould Tool Steel

Fushun are main manufacturer of tool steel for Hot Forging Mould.

 

What is Hot Forging Mould?

Hot forging moulds are specialized tooling systems designed for shaping metal components at elevated temperatures, typically above the material’s recrystallization temperature. These moulds incorporate sophisticated designs with carefully engineered cavities, flash gutters, and cooling channels to manage thermal stress and material flow. The mould assembly must withstand extreme temperatures and pressures while maintaining dimensional stability throughout repeated forging cycles.

 

The primary purpose of hot forging moulds is to produce complex-shaped components with excellent mechanical properties and material grain flow. They are extensively used in automotive, aerospace, and heavy industries to manufacture critical components like crankshafts, connecting rods, and turbine blades. Hot forging allows for significant material deformation with lower forming forces compared to cold forging, enabling the production of larger and more complex parts. The process can achieve near-net-shape components while optimizing material properties through controlled deformation and cooling.

 

The mould materials for hot forging applications contain carefully balanced combinations of alloying elements to withstand severe thermal and mechanical stresses. Premium grade hot-work tool steels are used, incorporating chromium, tungsten, molybdenum, and vanadium to provide optimal performance at elevated temperatures. These materials offer excellent hot hardness, thermal fatigue resistance, and toughness at high temperatures. The microstructure features thermally stable carbides that maintain hardness and wear resistance under repeated heating and cooling cycles. Special surface treatments and coatings are often applied to enhance thermal shock resistance and reduce friction during the forging process, while sophisticated heat treatment processes ensure optimal performance under extreme working conditions.

Hot Forging Mould Materials

—   4Cr2NiMoV
—   5Cr2NiMoVSi
H10 1.2365 4Cr3Mo3SiV
—   3Cr3Mo3W2V
    Ni53Cr19Mo3TiNb

 

Chemical Composition of Hot Forging Mould

Grade C Si Mn Cr W Mo Ni V
4Cr2NiMoV 0.35~0.45 ≤0.40 ≤0.40 1.80~2.20   0.45~0.60 1.10~1.50 0.10~0.30
5Cr2NiMoVSi 0.46~0.54 0.50~0.90 0.40~0.60 1.50~2.00   0.80~1.20 0.80~1.20 0.30~0.50
4Cr3Mo3SiV 0.35~0.45 0.80~1.20 0.25~0.70 3.00~3.75   2.00~3.00   0.25~0.75
3Cr3Mo3W2V 0.32~0.42 0.60~0.90 ≤0.65 2.80~3.30 1.20~1.80 2.50~3.00   0.80~1.20
Ni53Cr19Mo3TiNb ≤0.08 ≤0.35 ≤0.35 17.00~21.00   2.80~3.30 50.00~55.00  

 

Properties of Hot Forging Mould Steel

 

Grade Annealed HBW
4Cr2NiMoV ≤220
5Cr2NiMoVSi ≤255
4Cr3Mo3SiV ≤229
3Cr3Mo3W2V ≤255
Ni53Cr19Mo3TiNb ≤300

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

[email protected]

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x