DC53 High-Strength High-Toughness Cold Work Tool Steel

dc53 forged bar

A new high-quality Cr8 series cold work tool steel with high strength and toughness, showing significant improvement in overall performance compared to Cr12 series tool steels.

 

 

Composition Design:

Based on Cr8Mo2SiV steel composition, systematically optimized considering the effects of alloying elements on material strength and toughness, achieving enhanced strength-toughness balance to meet high-performance requirements.

 

Manufacturing Process:

  • – Vacuum refining
  • – Constant melting rate ESR under protective atmosphere
  • – Special forming process
  • – Spheroidizing annealing

 

Features

  • – High steel purity with minimal segregation
  • – Small difference between longitudinal and transverse properties
  • – Uniform carbide distribution
  • – Combined high strength and toughness

 

Applications

  • – Blanking dies, cold forming dies, drawing dies, forming rolls, punches, and cold pressing dies
  • – Precision blanking dies using wire-cut EDM and various stamping dies
  • – Dies for plastic deformation of difficult-to-machine materials
  • – High wear-resistant, high-hardness, high-toughness cold stamping dies
  • – Large-scale and precision dies

 

International Standards:

  • – China: CTDC53
  • – International GB: Cr8Mo2SiV
  • – Germany: K340
  • – ASSAB: Assab 88
  • – Japan: DC53

 

Chemical Composition (wt.%):

– Carbon (C): 0.90-1.20%

– Silicon (Si): 0.50-0.90%

– Manganese (Mn): ≤0.80%

– Chromium (Cr): 7.50-9.00%

– Molybdenum (Mo): 1.90-2.50%

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

 

CTDC53 Physical Properties:

 

1. Thermal Expansion Coefficient (10⁻⁶/°C)

– At 200°C: 12.6

– At 400°C: 13.2

– At 600°C: 13.7

 

2. Thermal Conductivity (W/m°C)

– At 25°C: 23.2

– At 200°C: 25.7

– At 400°C: 27.9

– At 600°C: 26.1

 

3. Specific Heat

– At 25°C: 460 J/kg°C

 

Note: All properties measured under standard conditions in professional testing facilities.

 

Other Tool Steel:

1.2344 H13 SKD61

1.2379 D2

1.2738 P20+Ni 718

1.2080 D3

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x