manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Alloy 716, N07716, Precipitation Hardened Superalloy

Alloy 716

Alloy 716 (625+) — Premium Precipitation Hardenable Nickel-Chromium-Molybdenum Superalloy

Product Description

FUSHUN METAL offers premium quality Alloy 716 (625+), a precipitation hardenable Nickel-Chromium-Molybdenum based superalloy that delivers an exceptional combination of high strength and superior corrosion resistance. This innovative material offers the high strength characteristics similar to Alloy 718 while providing the outstanding corrosion resistance comparable to Alloy 625. This unique combination makes Alloy 716 the ideal choice for demanding applications in oil and gas, chemical processing, and marine environments where both mechanical integrity and resistance to aggressive corrosive media are critical requirements.

The alloy’s exceptional properties are achieved through a carefully controlled chemical composition and optimized heat treatment process, resulting in a material that maintains its mechanical properties even in the harshest operating conditions. FUSHUN METAL supplies Alloy 716 in various product forms including round bars, flat bars, plates, and forgings, all manufactured to meet the most stringent industry specifications including ASTM B805, API 6A CRA, and NACE MR-0175/ISO 15156.

Standards and Specifications

Alloy 716 (625+) from FUSHUN METAL meets or exceeds the following industry standards and specifications:

Standard Designation
UNS N07716
ASTM B805
API 6A CRA
NACE MR-0175/ISO 15156
Tradename ALLOY 625+

Chemical Composition

FUSHUN METAL manufactures Alloy 716 (625+) with precise control of chemical composition according to the following requirements:

Element Content (%)
Nickel (Ni) 59.0 – 63.0
Chromium (Cr) 19.0 – 22.0
Molybdenum (Mo) 7.00 – 9.50
Niobium (Nb) + Tantalum (Ta) 2.75 – 4.00
Titanium (Ti) 1.00 – 1.60
Iron (Fe) Balance
Aluminum (Al) 0.35 Max
Carbon (C) 0.03 Max
Silicon (Si) 0.2 Max
Manganese (Mn) 0.2 Max
Phosphorus (P) 0.015 Max
Sulfur (S) 0.01 Max
Boron (B) 0.006 Max
Copper (Cu) 0.23 Max
Lead (Pb) 0.001 Max

Role of Key Alloying Elements

  • Nickel (59.0-63.0%): Forms the austenitic matrix and provides excellent resistance to corrosion, particularly in reducing environments. Also contributes to high-temperature stability and resistance to thermal cycling.
  • Chromium (19.0-22.0%): Provides resistance to oxidation and corrosion, particularly in oxidizing environments, through the formation of a protective oxide layer.
  • Molybdenum (7.00-9.50%): Significantly enhances resistance to pitting and crevice corrosion, especially in chloride-containing environments. Also contributes to solid solution strengthening.
  • Niobium (2.75-4.00%): Together with titanium, forms primary strengthening precipitates during age hardening heat treatment, contributing to the alloy’s high strength.
  • Titanium (1.00-1.60%): Forms strengthening precipitates and helps in age-hardening response. Also contributes to improved high-temperature properties.

Mechanical Properties

Alloy 716 (625+) from FUSHUN METAL exhibits exceptional mechanical properties in the solution annealed and aged condition:

Property Minimum Value Typical Value
0.2% Yield Strength 120,000 PSI (827 MPa) 125,000 PSI (862 MPa)
Tensile Strength 150,000 PSI (1034 MPa) 160,000 PSI (1103 MPa)
Elongation 20% 25%
Reduction of Area 35% 40%
Hardness (NACE Compliant) 32 HRC 32 – 43 HRC
Charpy V-Notch Impact @ -60°C 37 Joules 43 Joules

Physical Properties

FUSHUN METAL’s Alloy 716 (625+) demonstrates the following typical physical properties:

Property Value
Density 8.44 g/cm³ (0.305 lb/in³)
Melting Range 1290-1350°C (2354-2462°F)
Thermal Conductivity at 20°C 10.8 W/m·K (6.2 BTU/hr/ft/°F)
Electrical Resistivity 1.30 μΩ·m at 20°C
Coefficient of Thermal Expansion (20-100°C) 13.1 × 10⁻⁶ /°C (7.3 × 10⁻⁶ /°F)
Specific Heat 410 J/kg·K (0.098 BTU/lb/°F)
Young’s Modulus 205 GPa (29.7 × 10⁶ psi)

Key Advantages of Alloy 716 (625+)

Alloy 716 (625+) from FUSHUN METAL offers several significant advantages that make it a superior choice for demanding applications:

  • Optimal Combination of Strength and Corrosion Resistance: Delivers the high strength similar to Alloy 718 with the exceptional corrosion resistance of Alloy 625, offering the best of both worlds in a single material.
  • Superior Corrosion Resistance: Exceptional resistance to pitting, crevice corrosion, stress corrosion cracking, and general corrosion in both oxidizing and reducing environments.
  • NACE MR-0175/ISO 15156 Compliance: Fully certified for use in sour gas environments, making it ideal for oil and gas applications where H₂S is present.
  • High Mechanical Strength: The precipitation hardening capability provides excellent yield and tensile strength while maintaining good ductility.
  • Excellent High-Temperature Properties: Maintains its mechanical properties at elevated temperatures, making it suitable for high-temperature service.
  • Outstanding Fatigue Resistance: Superior resistance to cyclic loading, ensuring long service life in dynamic applications.
  • Good Fabricability: Can be machined, formed, and welded using conventional techniques with proper procedures.
  • Dimensional Stability: Minimal distortion during heat treatment and excellent dimensional stability during service.

Heat Treatment

FUSHUN METAL supplies Alloy 716 (625+) bar stock in the Solution Annealed and Aged condition as standard. Material may also be supplied in the Solution Annealed only condition upon request.

Standard Heat Treatment Process

  • Solution Annealing: 1010-1065°C (1850-1950°F), hold for sufficient time based on section thickness, followed by rapid cooling (water quenching).
  • Aging Treatment: Two-step aging process:
    • First Step: 720-760°C (1330-1400°F) for 8 hours
    • Furnace cool at 55°C (100°F) per hour to 620-660°C (1150-1220°F)
    • Second Step: Hold at 620-660°C (1150-1220°F) for 8 hours
    • Air cool to room temperature

This precise heat treatment schedule optimizes the precipitation hardening response to achieve the ideal combination of strength, ductility, and corrosion resistance in the final product.

Applications

Due to its exceptional combination of high strength and superior corrosion resistance, Alloy 716 (625+) from FUSHUN METAL is ideally suited for numerous demanding applications:

Oil and Gas Industry

  • Downhole components for sour service environments
  • Wellhead equipment and Christmas trees
  • Subsurface safety valves
  • Completion equipment
  • Flow control devices
  • Subsea equipment
  • Pressure-containing components

Chemical Processing

  • Process equipment for handling aggressive chemicals
  • Heat exchangers
  • Reaction vessels
  • Valves and pumps
  • Piping systems in corrosive environments

Marine Applications

  • Propeller shafts
  • Fasteners and hardware for seawater exposure
  • Offshore platform components
  • Marine exhaust systems

Aerospace and Defense

  • High-strength components requiring corrosion resistance
  • Structural elements in marine environments
  • Exhaust system components

Power Generation

  • Gas turbine components
  • Fasteners for high-temperature service
  • Heat recovery steam generator components

Available Product Forms

FUSHUN METAL provides Alloy 716 (625+) in various product forms to meet diverse manufacturing requirements:

Round Bars

Diameter Range Length Surface Condition
12mm – 300mm (0.5″ – 12″) Random or cut-to-length Black/As-forged, Rough-turned, Precision-ground, Polished

Flat Bars

Thickness Width Length
10mm – 100mm (0.4″ – 4″) 20mm – 200mm (0.8″ – 8″) Random or cut-to-length

Plates

Thickness Width Length
5mm – 50mm (0.2″ – 2″) Up to 1500mm (60″) Up to 6000mm (240″)

Forgings

Type Weight Range Condition
Open die forgings, rings, discs, blocks Up to 2000kg Solution annealed or solution annealed and aged

Corrosion Resistance

Alloy 716 (625+) from FUSHUN METAL offers outstanding corrosion resistance in a wide range of aggressive environments, making it an excellent choice for applications where material integrity is critical:

General Corrosion Resistance

Similar to Alloy 625, Alloy 716 demonstrates exceptional resistance to general corrosion in both oxidizing and reducing environments, including:

  • Mineral acids (sulfuric, phosphoric, nitric)
  • Organic acids
  • Alkaline solutions
  • Seawater and marine environments
  • Industrial atmospheres

Localized Corrosion Resistance

The high molybdenum content (7.00-9.50%) provides superior resistance to:

  • Pitting corrosion in chloride-containing environments
  • Crevice corrosion in stagnant conditions
  • Stress corrosion cracking

Sour Service Performance

Alloy 716 is fully compliant with NACE MR-0175/ISO 15156 specifications, making it suitable for service in oil and gas environments containing hydrogen sulfide (H₂S). The alloy demonstrates excellent resistance to:

  • Sulfide stress cracking (SSC)
  • Hydrogen-induced cracking (HIC)
  • Stress-oriented hydrogen-induced cracking (SOHIC)

High-Temperature Corrosion Resistance

The alloy also exhibits excellent resistance to various forms of high-temperature corrosion, including:

  • Oxidation at elevated temperatures
  • Carburization
  • Sulfidation
  • Hot corrosion (Type I and Type II)

Fabrication Guidelines

Alloy 716 (625+) can be fabricated using conventional techniques, with the following recommendations:

Machining

  • Alloy 716 has machinability similar to other nickel-based superalloys
  • Use rigid tooling setups to minimize chatter and deflection
  • Carbide tooling with positive rake angles is recommended
  • Lower cutting speeds compared to stainless steels are advised
  • Adequate cooling and lubrication should be maintained
  • Solution annealed condition is generally preferred for machining operations

Welding

  • Gas Tungsten Arc Welding (GTAW/TIG) is the preferred method for joining
  • Use matching filler metals (ERNiCrMo-3) or Alloy 625 filler metal
  • Maintain clean surfaces free from contamination before welding
  • Minimize heat input to prevent thermal distortion
  • Pre-weld solution annealing may be beneficial for thick sections
  • Post-weld heat treatment is recommended to restore corrosion resistance and mechanical properties

Forming

  • Perform forming operations in the solution annealed condition
  • Higher forces are required compared to austenitic stainless steels
  • Minimum bend radius should be at least 2-3 times the material thickness
  • Intermediate annealing may be necessary for severe forming operations
  • Age hardening heat treatment should be performed after all forming operations are complete

Surface Finishing

  • Standard grinding, polishing, and abrasive blasting techniques are effective
  • Avoid contamination with iron particles during surface finishing
  • Passivation treatments can enhance corrosion resistance
  • Electro-polishing can provide superior surface finish and corrosion performance

Quality Assurance

FUSHUN METAL maintains the highest standards of quality for Alloy 716 (625+):

  • Chemical Analysis: Each heat is analyzed using state-of-the-art spectrometers to ensure compositional compliance with specifications
  • Mechanical Testing: Comprehensive testing including tensile, hardness, and impact properties
  • Microstructural Examination: Proper grain size and precipitate distribution are verified through metallographic analysis
  • Non-Destructive Testing: Ultrasonic, magnetic particle, and liquid penetrant inspection as required by specifications
  • Corrosion Testing: Material is tested for resistance to specific corrosive environments when required
  • Dimensional Inspection: All products undergo thorough dimensional verification
  • Certification: Complete material test reports and certification documentation are provided with each shipment
  • Traceability: Full traceability from melt to final product is maintained

Comparative Advantages

Understanding how Alloy 716 (625+) compares to similar alloys helps in selecting the optimal material for specific applications:

Characteristic Alloy 716 (625+) Alloy 625 Alloy 718
Yield Strength 120 ksi min 60 ksi min 150 ksi min
Corrosion Resistance Excellent Excellent Good
Pitting Resistance Superior Superior Moderate
NACE MR-0175 Compliance Yes Yes Limited
Age Hardenability Yes No (standard grade) Yes
Maximum Service Temperature ~650°C (1200°F) ~980°C (1800°F) ~650°C (1200°F)
Optimal Application Area Corrosive environments requiring high strength Highly corrosive environments with moderate strength needs High-strength applications with moderate corrosion concerns

Why Choose FUSHUN METAL for Alloy 716 (625+)

Selecting FUSHUN METAL as your supplier for Alloy 716 (625+) provides numerous advantages:

  • Material Expertise: Our team of metallurgists and engineers has extensive experience with nickel-based superalloys and their applications
  • Manufacturing Excellence: State-of-the-art production facilities with stringent quality control measures ensure consistent material properties
  • Comprehensive Testing: All products undergo thorough testing to verify mechanical properties, dimensional accuracy, and corrosion resistance
  • Custom Solutions: Ability to tailor product specifications to meet specific application requirements
  • Technical Support: Expert assistance with material selection, heat treatment, and fabrication guidelines
  • Global Supply Capability: Worldwide distribution network ensures timely delivery
  • Industry Compliance: All products meet or exceed relevant industry standards including ASTM, API, and NACE specifications
  • Competitive Pricing: Excellent value proposition for premium superalloy products

Request Information

Contact FUSHUN METAL today to discuss your Alloy 716 (625+) requirements. Our technical team is ready to assist you with:

  • Detailed technical specifications
  • Custom size and property requirements
  • Fabrication recommendations
  • Application-specific material selection guidance
  • Price quotations and delivery schedules
  • Material certification and testing requirements

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x