manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

13-8PH 1.4534 Martensitic Precipitation-Hardening Stainless Steel

 

13-8PH 1.4534 Martensitic Precipitation-Hardening Stainless Steel

Premium Quality by FUSHUN METAL

Advanced Manufacturing Excellence

As a leading Chinese manufacturer of specialty stainless steels, FUSHUN METAL produces high-quality 13-8PH martensitic precipitation-hardening stainless steel through advanced double-melting processes including Vacuum Induction Melting followed by Vacuum Arc Remelting (VIM-VAR) or Electroslag Remelting (ESR) techniques. This premium alloy demonstrates exceptional strength, high hardness, superior toughness, and excellent corrosion resistance comparable to 304 stainless steel, with optimal performance achieved in the fully hardened condition.

Our 13-8 PH steel features outstanding transverse toughness properties through precise chemical composition control, low carbon content design, and vacuum melting technology, offering a wide range of mechanical properties through single precipitation hardening heat treatment. The material exhibits excellent weldability with helium gas shielding recommended for optimal results, and maintains corrosion resistance similar to standard austenitic grades.

Chemical Composition Analysis

Symbol Element Min % Max %
C Carbon 0.05%
Mn Manganese 0.10%
Si Silicon 0.10%
P Phosphorus 0.010%
S Sulfur 0.008%
Cr Chromium 12.25% 13.25%
Ni Nickel 7.50% 8.50%
Mo Molybdenum 2.00% 2.50%
N Nitrogen 0.010%
Al Aluminum 0.90% 1.35%
Fe Iron Balance

Heat Treatment Conditions

Condition Temperature
H950 950 °F ± 10 °F (510 °C ± 6 °C)
H1000 1000 °F ± 10 °F (538 °C ± 6 °C)
H1025 1025 °F ± 10 °F (552 °C ± 6 °C)
H1050 1050 °F ± 10 °F (566 °C ± 6 °C)
H1100 1100 °F ± 10 °F (593 °C ± 6 °C)
H1150 1150 °F ± 10 °F (621 °C ± 6 °C)

Mechanical Properties Performance

Condition Tensile Strength Yield 0.2% Offset Elongation (%in 2″) Reduction of Area Brinell Hardness Rockwell Hardness
Ann 175 ksi max 363 max
H950 220 ksi 205 ksi 10% 45% C45 min
H1000 205 ksi 190 ksi 10% 50% C45 min
H1025 185 ksi 175 ksi 11% 50%
H1050 175 ksi 165 ksi 12% 50% C40 min
H1100 150 ksi 135 ksi 14% 50% C34 min
H1150 135 ksi 90 ksi 14% 50% C30 min

Key Applications & Industries

Aerospace Components
High-performance aircraft structural parts and components
Injection Molding Equipment
Precision manufacturing tools and machinery
Waterjet Cutting Equipment
High-pressure cutting system components
Petrochemical Industries
Corrosion-resistant process equipment
Nuclear Industries
Critical nuclear facility components
Marine Engineering
High-performance marine applications

Our products are widely utilized in aerospace, marine engineering, petrochemical, and other high-performance applications requiring exceptional combinations of strength, toughness, and corrosion resistance, backed by our comprehensive production capabilities and stringent quality control systems.

Complete Product Range & Specifications

Available Product Forms

Product Forms Classification Specifications (mm)
Ingots Master alloy Φ70~280 mm
Ingots Φ360~700 mm
Forged Products Round bar Φ30~450 mm
Square bar 30~600 mm
Plate, disc, flange, ring According to your request
Rods & Bars Hot Rolled Φ8~200
Cold Drawn Φ1~60
Tubes Seamless OD:6~273 WT:1~30 L:500~10000
Welded According to your request
Fitting Wrought/forged Delivery according ASTM B16.9 B16.11
Wires Roll/straight Φ0.1~25 mm
Strip hot/cold roll T:0.10~3.5 W:200~400mm
Plate & Sheet Hot Rolled T:3~50mm W:400~2500mm L:1000~8000mm
Cold Rolled T:0.4~4mm W:400~1200mm L:1000~2200mm

International Standards & Specifications

Common Specifications:

• AMS 5629 Bars, Forgings, Wire, Extrusions

• AMS 5629/H1000 (produced & precipitation hardened to H1000 condition)

• AMS 5864 (Plate)

• ASTM A564 (Type XM-13 Bars, Wires, Shapes)

• ASTM A693 (Sheet, Plate, Strip)

• ASTM A705 (Forgings)

Common Trade Names:

• PH13-8Mo

• XM-13

• UNS S13800

• 1.4534

• X3CrNiMoAl13-8-2

• DMS 2100 Grade

• HMS 6-1105 REV A AMD 3

• ST0160LB0013 REV E

• ASTM F899-12B

• RMS-150 REV N

Comprehensive Heat Treatment Services

Heat treatment, which is one of the special processes in which the mechanical properties of the material are re-shaped and which requires high engineering knowledge and experience, has been serving for more than 20 years with FUSHUN METAL’s expert engineers. We have a huge range of heat treatment facilities that can make special processes on tool steel, mould steel, high speed steels, stainless steel, alloy steel, nickel alloy, etc.

Normalizing
Quenching and Tempering
Induction Hardening
Stress Relief Annealing
Protective Atmosphere Annealing
Solution Annealing
Aging
Vacuum Hardening

Advanced Machining Capabilities

FUSHUN METAL offers not only an optimum material in various forms, but also pre-machined and ready-to-install parts. We put extensive consulting know-how and modern machining facilities at the disposal of our customers.

Grounded
Turned
Polished
Borehole Drill
Shot Blast
Lathe Cutting
Bend Sawing

Comprehensive Quality Control

All production workflows at FUSHUN METAL are monitored, inspected and controlled – from material checking, from melting to casting, and from the internal, surface, dimensional and identity checks in the finishing shops of the rolling mills and forging shops or on the bright steel lines, all the way to mechanical and technological tests on specimens.

Yield Strength
Precise measurement of material strength properties
Ultimate Tensile Strength
Maximum stress material can withstand
Elongation
Ductility and flexibility testing
Hardness Test
Brinell, Vickers, Rockwell C testing methods
Metallographic Analysis
Grain size, structure, micro-cleanliness, and flaws
High Temperature Strength
Performance under elevated temperatures
Charpy-V Impact Test
Toughness and impact resistance evaluation
Eddy Current Testing (ET)
Non-destructive testing for defect detection

FUSHUN METAL – Your Trusted Steel Partner

Over 20 years of expertise in specialty stainless steel manufacturing with advanced production facilities and stringent quality control systems. We supply 13-8PH stainless steel in various forms including bars, wire, forgings, rings, extrusions, sheet, and plate materials conforming to AMS 5629 aerospace specifications.

Contact FUSHUN METAL Today

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]