manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

2.4694, Alloy 751, SUH751, N07751, Valve Nickel Alloy

 

2.4694 Alloy 751 SUH751 NiCr16Fe7TiAl N07751 Valve Alloy – Premium Age-Hardenable Valve Material

High-Temperature Resistant Valve Alloy for Advanced Gas Turbine and Industrial Valve Applications by FUSHUN SPECIAL STEEL

2.4694 Alloy 751 SUH751 NiCr16Fe7TiAl N07751 Valve Alloy Introduction and Applications

FUSHUN SPECIAL STEEL is a leading manufacturer of 2.4694 (Alloy 751, SUH751, NiCr16Fe7TiAl, N07751) age-hardenable valve alloy specifically engineered for demanding high-temperature valve applications up to 820°C. This premium valve alloy achieves exceptional strength through titanium, niobium, and aluminum precipitation hardening, making it ideal for gas turbine valves, industrial valve components, and high-stress valve applications.

As a dedicated manufacturer, FUSHUN SPECIAL STEEL specializes in producing high-quality 2.4694 Alloy 751 SUH751 valve alloy with optimized heat treatment conditions for enhanced precipitation hardening characteristics. Our advanced melting technologies ensure consistent quality and performance for large-volume production requirements in high-temperature valve manufacturing industries.

Primary SUH751 Valve Alloy High-Temperature Applications

  • Gas turbine valves operating up to 820°C (1,510°F)
  • Industrial valve components requiring high tensile strength up to 600°C
  • High-temperature valve fasteners and bolting elements
  • Aerospace valve systems with oxidation resistance requirements
  • Power plant valve assemblies for steam applications
  • Chemical processing equipment valves in corrosive environments

International Valve Alloy Designations and Standards

Standard Material Designation
EN 2.4694 NiCr16Fe7TiAl
UNS N07751
JIS SUH751
Common Name Alloy 751

International Recognition: 2.4694 Alloy 751 SUH751 is globally recognized across EN, UNS, and JIS standards, ensuring worldwide compatibility and acceptance in high-temperature valve manufacturing industries and aerospace applications as a premium age-hardenable valve alloy.

2.4694 Alloy 751 SUH751 Valve Alloy Chemical Composition

Ni % Cr % C % S % Mn % Si % Ti % Nb %
min 70 14-17 max 0.10 max 0.01 max 1 max 0.5 2-2.6 0.7-1.2
Cu % Fe % Al %
max 0.5 5-9 0.9-1.5

2.4694 Alloy 751 SUH751 Enhanced Valve Alloy Composition: High nickel content (min 70%) provides excellent valve corrosion resistance and strength. Chromium (14-17%) ensures oxidation resistance. Titanium (2-2.6%), niobium (0.7-1.2%), and aluminum (0.9-1.5%) enable precipitation hardening for superior valve performance at high temperatures.

SUH751 Valve Alloy Physical Properties

Property Value
Density 8.2 g/cm³ at 20°C
Melting Range 1,390-1,430°C
Magnetic Permeability at 20°C 1.0035
Curie Temperature -223°C (-369°F)

2.4694 Alloy 751 SUH751 Mechanical Properties for Valve Applications

Condition: Solution-annealed and precipitation hardened valve alloy properties

Temperature Yield Strength
(MPa)
Tensile Strength
(MPa)
Elongation
(%)
20°C (68°F) 716 1080 24
200°C (392°F) 670 1020 27
600°C (1112°F) 660 912 25
700°C (1292°F) 660 861 14

2.4694 Alloy 751 SUH751 Valve Performance: Exceptional strength retention at elevated temperatures makes this valve alloy ideal for gas turbine and industrial valve applications. High tensile strength of 1080 MPa at room temperature combined with excellent strength retention up to 700°C ensures reliable valve performance in demanding high-temperature service conditions.

SUH751 Key Characteristics for Valve Applications

High-Temperature Valve Alloy Characteristics

  • High tensile strength up to 600°C (1,110°F) for valve applications
  • High creep and fatigue strength up to 820°C (1,510°F)
  • High oxidation resistance up to 980°C (1,795°F)
  • Excellent mechanical properties in low temperature environments
  • Good corrosion resistance in high and low temperatures and high resistance against stress corrosion
  • Good weldability for valve manufacturing (resistance and fusion welding)

SUH751 Heat Treatment for Valve Manufacturing

Solution Annealing

Temperature: 1080-1120°C

Cooling: Air or water quenching

Purpose: Optimal valve alloy structure

Precipitation Hardening

Temperature: 700-750°C

Duration: 16-20 hours

Cooling: Air cooling

Age-Hardening Process for Optimal Valve Performance

The two-step heat treatment optimizes 2.4694 Alloy 751 SUH751 valve alloy for demanding valve applications. Solution annealing dissolves precipitates, while precipitation hardening develops fine titanium, niobium, and aluminum precipitates that provide exceptional strength and thermal stability for valve components operating up to 820°C.

Processing Types We Provide

Hot Rolled

Premium hot rolled 2.4694 Alloy 751 SUH751 valve alloy with exceptional dimensional accuracy and superior mechanical properties for valve manufacturing. Our manufacturing process ensures consistent precipitation hardening response for optimal valve performance.

Hot Forged

Precision hot forged components with optimized grain structure for critical SUH751 valve alloy applications. As a manufacturer, we control the entire forging process for superior gas turbine and high-temperature valve components.

Available Shapes for SUH751 Valve Manufacturing

Round Bars

Precision round bars for SUH751 valve stem manufacturing

Flat Bars

High-quality flat bars for valve head manufacturing

Plates

Heavy plates for large valve component production

Wire

Precision wire for specialized valve applications

Available Sizes and Custom Manufacturing

Standard Inventory Sizes

FUSHUN SPECIAL STEEL maintains comprehensive inventory of standard 2.4694 Alloy 751 SUH751 valve alloy sizes for immediate delivery to gas turbine and industrial valve manufacturers. Our extensive stock ensures rapid response to urgent production requirements for large-volume orders.

Request our detailed stock list and competitive pricing for bulk SUH751 valve alloy orders.

Custom Size Manufacturing

Beyond standard dimensions, FUSHUN SPECIAL STEEL offers comprehensive custom manufacturing services for specialized SUH751 valve alloy applications with large-volume requirements for gas turbine and aerospace valve manufacturers.

Consult our engineering team for custom production capabilities and lead times.

FUSHUN SPECIAL STEEL Manufacturing Advantages

Advanced Melting Technology

We operate VIM, ESR, and VAR technologies, ensuring ultra-clean 2.4694 Alloy 751 SUH751 valve alloy production with precise titanium, niobium, and aluminum control for consistent precipitation hardening performance in valve applications.

In-House Heat Treatment

Our heat treatment facilities ensure stable quality and fast delivery times for SUH751 valve materials. Complete control over solution annealing and precipitation hardening processes guarantees optimal valve performance up to 820°C.

Precision Finishing Services

We provide in-house turning and grinding services for SUH751 valve alloy products, delivering ready-to-use valve components with superior surface finish and dimensional accuracy for gas turbine applications.

Large-Volume Valve Manufacturing

As a leading manufacturer, we welcome large-volume orders for 2.4694 SUH751 valve alloy and offer competitive pricing for bulk requirements for gas turbine and aerospace valve manufacturing projects.

Leading 2.4694 Alloy 751 SUH751 Valve Alloy Manufacturer

FUSHUN SPECIAL STEEL is your premier manufacturer for 2.4694 Alloy 751 SUH751 NiCr16Fe7TiAl N07751 age-hardenable valve alloy. We deliver advanced precipitation hardening solutions for demanding gas turbine and industrial valve applications with large-volume manufacturing capabilities up to 820°C service temperature.

Experience the SUH751 valve alloy advantage – contact our team today.

Ready for 2.4694 Alloy 751 SUH751 Valve Alloy Excellence?

Join gas turbine and aerospace manufacturers worldwide who trust FUSHUN SPECIAL STEEL for premium 2.4694 SUH751 age-hardenable valve alloy solutions. As your dedicated manufacturer, we provide advanced precipitation hardening technology with large-volume manufacturing capabilities for high-temperature valve applications up to 820°C.

Contact our SUH751 valve alloy specialists today for technical consultation and competitive bulk pricing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x