Introduction and Applications

961 stainless steel, also known as 3И961, is a premium martensitic heat-resistant stainless steel originally developed in the Soviet Union. This high-performance alloy is designated as S47310 under UNS numbering system, with Chinese designations including 13Cr11Ni2W2MoV (new standard) and 1Cr11Ni2W2MoV (former standard). As a professional stainless steel manufacturer, FUSHUN SPECIAL STEEL provides this material with guaranteed quality and competitive pricing for bulk orders.

Key Applications

Aerospace Components

Aircraft engine compressor blades, turbine discs, and structural components operating at temperatures up to 600°C.

High-Temperature Fasteners

Bolts, studs, and nuts for power generation equipment, petrochemical plants, and industrial turbines requiring excellent creep resistance.

Chemical Composition

The carefully balanced chemical composition of 961 stainless steel ensures optimal high-temperature strength and corrosion resistance. FUSHUN SPECIAL STEEL maintains strict control over all elements through advanced melting processes.

C Cr Ni W Mo V Si Mn
0.10-0.16 10.5-12.0 1.50-2.00 1.50-2.00 0.35-0.50 0.18-0.30 ≤0.60 ≤0.60

Note: P ≤0.030%, S ≤0.020%. All values in weight percentage.

Mechanical Properties

961 stainless steel exhibits exceptional mechanical properties after proper heat treatment, making it ideal for demanding high-temperature applications. The following properties are typical values after standard quenching and tempering.

Property Value Unit
Tensile Strength (Rm) ≥1080 MPa
Yield Strength (Rp0.2) ≥835 MPa
Elongation (A) ≥10 %
Reduction of Area (Z) ≥40 %
Impact Energy (KV) ≥39 J
Hardness 32-40 HRC

High-Temperature Properties (at 600°C)

Tensile Strength at 600°C ≥590 MPa
Yield Strength at 600°C ≥490 MPa

Heat Treatment

Proper heat treatment is essential to achieve the optimal mechanical properties of 961 stainless steel. FUSHUN SPECIAL STEEL offers in-house heat treatment services with precise temperature control and documentation.

Quenching

Temperature: 1000-1050°C

Cooling: Oil quenching or air cooling

Tempering

Temperature: 620-680°C

Cooling: Air cooling, double tempering recommended

Annealing (for machining)

Heat to 850-880°C, hold for adequate time, then furnace cool to 500°C, followed by air cooling. Annealed hardness: ≤255 HB.

Equivalent Standards and Designations

961 stainless steel corresponds to various international standards. FUSHUN SPECIAL STEEL can supply material certified to customer-specified standards.

Standard Designation
USA (ASTM/UNS) ASTM A473 S47310, UNS S47310
China (GB) 13Cr11Ni2W2MoV (new), 1Cr11Ni2W2MoV (former)
Russia (GOST) 3И961 (Original designation)
Europe (EN/DIN) Similar to X12CrNiWMoV12-2-2
Japan (JIS) Similar to SUH616

Available Forms and Sizes

As a specialized steel manufacturer, FUSHUN SPECIAL STEEL produces 961 stainless steel through hot rolling and hot forging processes in multiple product forms.

Hot Rolled Products

Round Bar: Ø20mm – Ø200mm
Flat Bar: Thickness 10mm – 80mm
Plate: Thickness 8mm – 100mm
Wire Rod: Ø5.5mm – Ø25mm

Hot Forged Products

Forged Round: Ø150mm – Ø800mm
Forged Flat: Thickness 80mm – 500mm
Forged Block: Custom dimensions
Forged Ring: Custom specifications

Custom Sizes Available: For special dimension requirements beyond standard sizes, please contact our sales team. FUSHUN SPECIAL STEEL welcomes bulk orders and can accommodate custom specifications for large volume purchases.

Why Choose FUSHUN SPECIAL STEEL

As an integrated special steel manufacturer, we control every step of production from melting to final processing, ensuring consistent quality and competitive pricing for our customers worldwide.

Advanced Melting Capabilities

In-house ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) for producing premium-grade steel with superior cleanliness and homogeneity.

Integrated Heat Treatment

Complete in-house heat treatment facilities with precise temperature control, ensuring consistent mechanical properties and full traceability documentation.

Surface Finishing Services

Turning (peeled) and grinding services available in-house, reducing your processing time and costs while ensuring dimensional accuracy.

Fast Delivery & Bulk Orders

Vertical integration enables shorter lead times. We welcome large volume orders and provide competitive pricing for long-term partnerships.

Request a Quote for 961 Stainless Steel

FUSHUN SPECIAL STEEL is your reliable manufacturer for high-quality 961 martensitic heat-resistant stainless steel. Contact us today for pricing on bulk orders, custom sizes, and technical specifications.


About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x