What is AM355 Stainless Steel?

AM355 is a martensitic precipitation hardening stainless steel that combines exceptional strength with excellent corrosion resistance. This chromium-nickel-molybdenum alloy is specifically engineered for applications demanding superior mechanical properties at both ambient and elevated temperatures. As a professional manufacturer, FUSHUN SPECIAL STEEL produces AM355 steel with strict quality control to meet the most demanding aerospace and industrial specifications.

The unique combination of high chromium (15.0-16.0%) and molybdenum (2.50-3.25%) content provides AM355 with outstanding resistance to stress corrosion cracking and general corrosion in harsh environments. The nitrogen addition (0.07-0.13%) enhances strength and improves austenite stability during processing.

AM355 Steel Applications

Aerospace Industry

AM355 is widely used in aerospace applications including aircraft structural components, landing gear parts, turbine engine components, and fasteners. Its high strength-to-weight ratio and fatigue resistance make it ideal for critical flight safety components.

Industrial Applications

Beyond aerospace, AM355 serves in oil and gas equipment, nuclear power plant components, marine hardware, and high-performance valve stems. The alloy performs exceptionally well in environments where both high strength and corrosion resistance are required. Contact FUSHUN SPECIAL STEEL for customized AM355 solutions.

AM355 Chemical Composition (%)

C Si Mn P S Cr Ni Mo N
0.10-0.15 ≤0.50 0.50-1.25 ≤0.025 ≤0.015 15.0-16.0 4.0-5.0 2.50-3.25 0.07-0.13

Note: The above composition is produced and guaranteed by FUSHUN SPECIAL STEEL as a direct manufacturer.

AM355 Mechanical Properties

Typical Properties After Heat Treatment (SCT850 Condition)

Property Value
Tensile Strength ≥1170 MPa (170 ksi)
Yield Strength (0.2%) ≥1000 MPa (145 ksi)
Elongation ≥10%
Reduction of Area ≥35%
Hardness 35-42 HRC

AM355 steel exhibits excellent strength retention at temperatures up to 425°C (800°F). The alloy also demonstrates superior fatigue resistance and notch toughness compared to conventional martensitic stainless steels.

AM355 Heat Treatment

Solution Treatment

Heat to 1010-1065°C (1850-1950°F), hold for adequate time depending on section size, then cool rapidly. Oil quenching or air cooling may be used depending on section thickness and required properties.

Sub-Zero Treatment

Cool to -73°C (-100°F) or lower for 3 hours minimum. This treatment transforms retained austenite to martensite and is essential for achieving maximum strength and hardness.

Aging Treatment

Age at 425-565°C (800-1050°F) for 3-4 hours, followed by air cooling. The specific aging temperature depends on the desired balance of strength, ductility, and corrosion resistance. FUSHUN SPECIAL STEEL provides complete heat treatment services with in-house facilities.

AM355 Equivalent Grades & Standards

Standard Designation
USA (ASTM/AMS) AMS 5743, AMS 5547, AMS 5549, AMS 5745, UNS S35500
Europe (EN/DIN) 1.4959, X8CrNiMoN15-5-3
Japan (JIS) –
China (GB) 0Cr15Ni5Mo3N

AM355 Product Forms & Available Sizes

As a vertically integrated steel manufacturer, FUSHUN SPECIAL STEEL offers AM355 in multiple product forms through hot rolling and hot forging processes:

Product Form Available Sizes
Round Bar (Hot Rolled) Φ20mm – Φ200mm
Round Bar (Hot Forged) Φ200mm – Φ800mm
Flat Bar Thickness: 20mm – 300mm, Width: 50mm – 600mm
Plate Thickness: 10mm – 200mm
Wire Φ5.5mm – Φ20mm

Special sizes available on request. Contact our sales team for custom dimensions and specifications. We welcome bulk orders from industrial buyers worldwide.

Why Choose FUSHUN SPECIAL STEEL for AM355?

In-House Melting Capability

We operate advanced melting facilities including ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) for producing premium-grade AM355 steel with superior cleanliness and homogeneity.

Complete Heat Treatment Services

Our in-house heat treatment facilities ensure consistent mechanical properties and reliable quality. We control the entire process from melting to final heat treatment for optimal results.

Precision Machining Available

We provide turned and ground bar finishing services, saving our customers time and reducing their processing costs. Get ready-to-use AM355 steel products directly from our factory.

Fast Delivery & Stable Quality

As a direct manufacturer with integrated production, we offer short lead times and consistent quality for every order. Bulk orders are especially welcome.

Order AM355 Steel from FUSHUN SPECIAL STEEL Today

As a leading AM355 steel manufacturer, we provide competitive pricing for bulk orders with reliable quality and fast delivery. Contact us for quotations and technical support.

Request a Quote

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x