manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

MP35N 2.4999 Superalloy Nickel-Cobalt-Chromium-Molybdenum

 



MP35N Superalloy | High-Strength Nickel-Cobalt-Chromium-Molybdenum Alloy | FUSHUN SPECIAL STEEL

MP35N 2.4999 Superalloy – Ultra-High Strength Nickel-Cobalt-Chromium-Molybdenum Alloy | FUSHUN SPECIAL STEEL

Introduction & Applications

MP35N is a premium nonmagnetic nickel-cobalt-chromium-molybdenum superalloy renowned for its exceptional combination of ultra-high tensile strength, outstanding ductility, and superior corrosion resistance. As a professional manufacturer, FUSHUN SPECIAL STEEL produces MP35N through advanced vacuum induction melting (VIM) followed by vacuum arc remelting (VAR) to ensure the highest quality standards.

This alloy can achieve tensile strength up to 300 ksi (2068 MPa) through cold work hardening, phase transformation, and aging processes. MP35N demonstrates exceptional resistance to sulfidation, high-temperature oxidation, and hydrogen embrittlement, making it ideal for the most demanding applications.

Key Applications

Aerospace & Energy

  • High-strength fasteners and springs
  • Gas and oil well service components
  • Sour environment equipment
  • Turbine engine components

Medical & Industrial

  • Orthopedic implants and surgical instruments
  • Dental and cardiovascular devices
  • Nonmagnetic electrical components
  • Precision instrument parts

MP35N Chemical Composition

Applicable specifications: AMS 5758, AMS 5844, AMS 5845, ANSI/ASTM F562 | UNS R30035

Element Ni Co Cr Mo Fe Ti
Content (%) 33.00-37.00 Balance 19.00-21.00 9.00-10.50 Max 1.00 Max 1.00
Element Mn Si C S P B
Content (%) Max 0.15 Max 0.15 Max 0.025 Max 0.010 Max 0.015 Max 0.015

MP35N Mechanical Properties

Room Temperature Tensile Properties

Condition Cold Reduction (%) 0.2% Yield Strength (ksi/MPa) Ultimate Tensile Strength (ksi/MPa) Elongation (%) Hardness (HRC)
Work Strengthened 25 150 / 1034 170 / 1172 28 34
35 154 / 1062 194 / 1336 22 42
55 205 / 1413 265 / 1827 12 47
65 235 / 1620 280 / 1931 11 50
Work Strengthened + Aged (1000°F/538°C, 4hrs) 25 175 / 1207 186 / 1282 24 39
45 251 / 1731 257 / 1772 12 46
53 290 / 1999 300 / 2068 10 50-51

Elevated Temperature Tensile Properties (Aged 1050°F/565°C, 4 hours, Air Cooled)

Test Temperature (°F/°C) 0.2% Yield Strength (ksi/MPa) Ultimate Tensile Strength (ksi/MPa) Elongation (%) Reduction of Area (%)
Room 285 / 1965 294 / 2027 10.0 46
400 / 204 248 / 1710 260 / 1793 8.0 44
600 / 316 236 / 1627 250 / 1724 8.0 41
800 / 426 225 / 1551 240 / 1655 4.0 8

Fatigue Strength (R.R. Moore Bending)

Condition 10⁶ Cycles (ksi/MPa) 10⁷ Cycles (ksi/MPa) 10⁸ Cycles (ksi/MPa)
Cold Drawn & Aged to 220 ksi (1517 MPa) 100 / 689 90 / 620 88 / 606
Cold Drawn & Aged to 265 ksi (1827 MPa) 108 / 744 99 / 682 97 / 668

Note: MP35N is included in NACE MR-01-75 to a maximum hardness of 35 HRC, or 51 HRC in specific cold reduced plus aged conditions for sour service environments.

MP35N Heat Treatment

Annealing

MP35N should be annealed at 1900-1950°F (1038-1066°C) for 1 to 4 hours, followed by air cooling. This process restores ductility for subsequent forming operations.

Aging

After work hardening, MP35N can be aged at 1000-1200°F (538-649°C) for increased strength. For optimum properties, cold worked MP35N should be aged at 1000-1100°F (538-593°C) for 4 hours, then air cooled.

Important: The alloy will respond to aging only if first work strengthened. No increase in strength will result from aging annealed material. Service temperatures up to 750°F (399°C) are suggested for the fully work hardened condition.

MP35N Equivalent Standards & Specifications

Standard Specification/Designation
UNS R30035
ASTM (USA) ASTM F562
AMS (USA) AMS 5758, AMS 5844, AMS 5845
ISO (International) ISO 5832-6 (Surgical Implants)
NACE MR-01-75 (Sulfide Stress Cracking Resistant)
DIN/EN (Europe) 2.4999, NiCo20Cr20Mo

MP35N Product Forms & Supply Range

As a professional manufacturer, FUSHUN SPECIAL STEEL supplies MP35N superalloy in various forms through hot rolling and hot forging processes. We welcome bulk orders and can accommodate special size requirements.

Product Form Process Size Range
Round Bars Hot Rolled / Hot Forged Ø15mm – Ø350mm
Flat Bars Hot Rolled / Hot Forged Thickness: 10mm – 150mm
Plates Hot Rolled Thickness: 6mm – 100mm
Wire / Wire Rod Hot Rolled Ø5.5mm – Ø25mm
Billets Hot Forged Ø100mm – Ø500mm

* Custom sizes and special requirements are available upon request. Contact us for your specific needs.

Why Choose FUSHUN SPECIAL STEEL as Your MP35N Manufacturer?

🔥 In-House Melting Capabilities

We operate our own ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) facilities to produce premium quality MP35N superalloy with exceptional cleanliness and homogeneity.

⚙️ Complete Heat Treatment

Our in-house heat treatment facilities ensure consistent quality and precise property control. We can deliver MP35N in annealed, work hardened, or aged conditions per your specifications.

✨ Precision Finishing Services

We offer bright turning and centerless grinding services in-house. This saves our customers time and reduces costs by eliminating the need for secondary processing at downstream facilities.

🚀 Fast Delivery & Bulk Orders

As a direct manufacturer, we offer stable quality, competitive pricing, and fast lead times. We especially welcome large volume orders and can establish long-term supply agreements.

Ready to Order MP35N Superalloy?

As a leading manufacturer of specialty steel and superalloys, FUSHUN SPECIAL STEEL is your trusted partner for high-quality MP35N. Contact our technical team today to discuss your requirements. Bulk orders and custom specifications are welcome!

Visit us at: www.fushunspecialsteel.com

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x