Hastelloy C2000 Alloy (UNS N06200) — Composition, Properties, Equivalent Grades & Supplier

Hastelloy C2000 (UNS N06200, W.Nr. 2.4675) is a copper-bearing nickel-chromium-molybdenum alloy developed by Haynes International, engineered to deliver exceptional corrosion resistance across both oxidizing and reducing acid environments within a single chemistry. Its balanced composition of approximately 23% chromium, 16% molybdenum, and 1.6% copper achieves the broadest corrosion coverage among all wrought C-family alloys, resisting sulfuric acid, hydrochloric acid, hydrofluoric acid, and chloride-induced pitting and crevice corrosion. The alloy serves as a universal solution for mixed-acid chemical processing where process streams alternate between oxidizing and reducing regimes.

Hastelloy C2000 alloy bars and forgings
Hastelloy C2000 bars and forgings by FUSHUN METAL

FUSHUN METAL manufactures Hastelloy C2000 using VIM, VAR, and PESR triple-melt pathways to achieve ultra-low gas content (H ≤ 0.9 ppm, O ≤ 13 ppm) and superior micro-cleanliness. Every heat undergoes precise composition control ensuring copper stays in solid solution and carbon remains below 0.01%, effectively preventing grain-boundary carbide precipitation that would otherwise compromise corrosion resistance in the heat-affected zone. Certified to ISO 9001:2015 and AS9120B, FUSHUN METAL delivers full material traceability with 100% ultrasonic testing per ASTM A388, positive material identification via XRF, and third-party inspectable MTR documentation on every shipment.

Equivalent Grades of Hastelloy C2000

Similar Alloy UNS / ASTM W.Nr. / DIN EN JIS Key Feature
Hastelloy C2000 N06200 (B574/B575/B622) 2.4675 / NiCr23Mo16Cu NiCr23Mo16Cu NW06200 Cu-bearing; broadest acid coverage
Hastelloy C-276 N10276 (B574/B575/B622) 2.4819 / NiMo16Cr15W NiMo16Cr15W NW0276 No Cu; W-bearing; industry benchmark
Hastelloy C-22 N06022 (B574/B575/B622) 2.4602 / NiCr21Mo14W NiCr21Mo14W NW6022 Higher Cr; superior oxidizing resistance
Alloy 59 N06059 (B574/B575/B622) 2.4605 / NiCr23Mo16 NiCr23Mo16 NW6059 No Cu; best thermal stability
Inconel 686 N06686 (B574/B575/B622) 2.4606 / NiCr21Mo16W NiCr21Mo16W NW6686 Highest PREN; W+Mo combination

Applications of Hastelloy C2000

Chemical Processing

Sulfuric acid reactors, hydrochloric acid heat exchangers, distillation columns, mixed-acid piping systems, centrifugal pumps, control valves, and pressure vessels handling alternating oxidizing/reducing process streams.

Pharmaceutical & Fine Chemicals

CIP-capable reactors, vacuum dryers, solvent recovery condensers, and high-purity transfer lines exposed to organic acids, halogenated solvents, and aggressive cleaning chemistries.

Pollution Control

FGD absorber vessels, mist eliminators, slurry circulation piping, stack liners, and quench sections in waste incineration and coal-fired power plant scrubbers.

Oil & Gas / Marine

Sour gas wellhead components, subsea umbilical tubing, seawater-cooled heat exchangers, desalination brine heaters, and offshore platform piping exposed to H2S and chloride-laden environments.

Pulp & Paper

Bleach plant washers, chlorine dioxide stages, digesters, and acid-handling equipment exposed to hot chlorinated and acidic pulping liquors.

Energy & Geothermal

Geothermal brine handling equipment, supercritical water oxidation reactors, and waste-to-energy heat recovery boilers facing high-temperature acidic condensate corrosion.

FUSHUN METAL Supply Range for Hastelloy C2000

Hastelloy C2000 rolled plates and sheets
Hastelloy C2000 rolled bars and flats supplied by FUSHUN METAL

Rolled Round Bars: Diameter 6 mm to 300 mm, solution-annealed with centerless-ground surface finish (h9/h10 tolerance), supplied in lengths up to 6 meters. Typical stock: 10-200 mm.

Rolled Flat Bars: Thickness 3 mm to 120 mm, width 20 mm to 800 mm, length up to 6 meters. Hot-rolled and cold-finished options with pickled or bright surface finish.

Forged Round Bars: Diameter 50 mm to 800 mm, open-die forged from ESR ingots at 1040-1200 deg C with controlled grain refinement to ASTM No. 5-7, solution-annealed and rough-turned.

Forged Flat Bars / Blocks: Thickness 15 mm to 500 mm, width 100 mm to 2000 mm, single-piece weight up to 5 metric tons. Suitable for machined components, tube sheets, and flanges.

Plates & Sheets: Hot-rolled plates 4.0 mm to 60 mm thick, width up to 2500 mm. Cold-rolled sheets 0.5 mm to 3.0 mm thick, width up to 1500 mm. UT-tested per ASTM A578.

Seamless Tubes & Pipes: Outer diameter 6 mm to 325 mm, wall thickness 0.5 mm to 30 mm. Cold-pilgered/cold-drawn with hydrogen-annealed bright surface, 100% ECT plus hydrostatic test per ASTM B622.

Chemical Composition of Hastelloy C2000

Element Ni Cr Mo Cu Fe Co C Mn Si Al P S
Min Bal. 22.0 15.0 1.3 — — — — — — — —
Max Bal. 24.0 17.0 1.9 3.0 2.0 0.01 0.50 0.08 0.50 0.025 0.010

Composition per ASTM B574 / B575 for UNS N06200, weight percent. FUSHUN METAL operates within tighter internal targets: Cr 22.5-23.5%, Mo 15.5-16.5%, Cu 1.5-1.8%, verified by optical emission spectrometry on every heat.

Mechanical Properties of Hastelloy C2000

Solution-Annealed Condition (1121-1149 deg C / 2050-2100 deg F, Water Quenched)

Property Tensile Strength Yield Strength (0.2%) Elongation Hardness Elastic Modulus Density Melting Range
Min. Req. 690 MPa 283 MPa 45% ≤100 HRB 206 GPa 8.50 g/cm3 1328-1358 deg C
Typical 750-780 MPa 350-390 MPa 55-65% 88-95 HRB — — —

Values per ASTM B574/B575. FUSHUN METAL performs room-temperature tensile testing per ASTM E8 on every production lot, with hardness verification per ASTM E18. Grain size is maintained at ASTM 5-7 through controlled forging and solution-annealing cycles.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x