ASTM A108 is the specification for cold finished carbon and alloy steel bars. Where A29 sets the general requirements for hot wrought bars, A108 covers what changes when the bar is cold drawn, turned, ground or polished afterwards: the surface, the straightness, the dimensional tolerance and the mechanical properties in each delivered condition.

What A108 covers

  • Forms — rounds, squares, hexagons and flats, in bar lengths.
  • Finishing routes — cold drawn, turned and polished, turned ground and polished, and ground stock.
  • Conditions — cold drawn, cold drawn and stress relieved, annealed, normalised, and quenched and tempered.
  • Requirements — chemical composition, mechanical properties by condition and size, surface quality, straightness, and dimensional tolerances.

How A108 relates to the other bar specifications

Specification What it fixes
ASTM A29 General requirements for hot wrought carbon and alloy bars — chemistry, inspection, marking
ASTM A108 Cold finished bars — finish, tolerance, straightness, mechanical properties by condition
ASTM A304 End quench hardenability (H band) requirements
ASTM A322 Chemical composition of the standard alloy grades

In practice a cold finished bar order cites two documents: A108 for the finish and tolerance, plus A29 or A322 for the grade chemistry.

What to put on the purchase order

  • The grade, by its AISI/SAE number or the A29/A322 designation.
  • The finishing route — cold drawn is not the same product as turned, ground and polished, and the price differs accordingly.
  • The condition: cold drawn as-is, stress relieved, annealed or quenched and tempered.
  • The size and the tolerance class. Cold drawn bar holds a much tighter tolerance than hot rolled, but the tolerance band still depends on diameter.
  • Straightness and surface requirements, especially if the bar goes straight into a bar feeder or a grinder.

Where cold finished bar is used

Shafts, spindles, pins, hydraulic rod, fasteners and any part that is machined from bar without a prior turning operation. The point of paying for cold finishing is to remove a roughing pass and to get a consistent diameter into the machine.

Download the standard

ASTM A108 — Standard Specification for Steel Bar, Carbon and Alloy, Cold-Finished (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x