manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

ASTM A322 1991 Standard Specification for Steel Bars, Alloy, Standard Grades

ASTM A322 gives the chemical composition requirements for standard alloy steel bars. It is a chemistry-only specification: it lists the grade designations and the ladle analysis ranges, and it does not by itself set mechanical properties. Those come from the purchase order, from A29 general requirements, or from a hardenability specification such as A304.

What A322 covers

  • Chemical composition ranges for the standard alloy bar grades, by ladle analysis.
  • The 13xx manganese, 40xx molybdenum, 41xx chromium-molybdenum, 43xx and 47xx nickel-chromium-molybdenum, 50xx chromium, 51xx chromium, 61xx chromium-vanadium, 81xx, 86xx, 87xx, 88xx, 92xx and 93xx nickel-chromium-molybdenum families.
  • Reference to A29 for the general requirements — inspection, tolerances, marking and the test methods behind the chemistry.

What it does not cover: mechanical properties, hardenability bands, heat treatment, or surface condition. A bar ordered “to A322 4140” is a chemistry commitment only.

A322, A29 and A304 — which one do you cite

If you need Cite
Just the chemistry of a standard alloy grade A322
Chemistry plus general bar requirements (tolerance, marking, inspection) A29 + A322
A guaranteed hardenability band A304 (H grades)
Cold finished bar rather than hot wrought A108

The grades buyers ask for most

4130, 4140, 4340, 8620, 8630, 9310 and the 41xx chromium-molybdenum family. All of them are defined chemically in A322 and are stocked as bar and forging stock; the equivalent European and Japanese designations are listed on the individual grade pages.

Download the standard

ASTM A322 — Standard Specification for Steel Bars, Alloy, Standard Grades (PDF)

Related reading

  • ASTM A29 — general requirements that A322 depends on.
  • ASTM A304 — when you need a hardenability band, not just chemistry.
  • ASTM A108 — the cold finished bar specification.
  • AISI 4140 — the most common grade in this family.
  • AISI 4130 — the lower-carbon member of the same family.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x