manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

ASTM A313 Stainless Steel Spring Wire

Stainless steel · Spring wire · A313 wire

ASTM A313 Stainless Steel Spring Wire

A313 wire supplied with an EN 10204 3.1 certificate and full traceability.

0.20–8.00 mm
Wire diameter
1,300–1,900 MPa
Tensile range
302 / 304 / 316
Spring grades
EN 10204 3.1
Every lot

At a glance

Table 1 — A313 wire at a glance

Item Detail
Designations A313 wire
Standards EN / ASTM — named on the certificate
Delivery condition Annealed or quenched and tempered
Supply range spring wire 0.20–8.00 mm; coil 0.20–8.00 mm
Typical use Engineering components
Certificate EN 10204 3.1 with chemistry and mechanical properties

Why A313 wire is bought by tensile, not by grade name

A313 wire is cold drawn to the spring temper: the tensile is bought by cold reduction, not by alloying. 302 gives the highest tensile of the three grades, 316 the best corrosion resistance, 304 the usual compromise.

The grade matters less than the temper and the surface. Two coils of 304 at the same diameter can differ by 300 MPa depending on the drawing pass, so the tensile band belongs on the drawing.

For a spring that will be stress relieved after coiling, specify the relief temperature with the order; above 350 °C the cold work is drawn out and the spring loses load.

Where A313 wire orders go wrong

What buyers get wrong
  • Buying tempered strip and forming a tight radius; the strip cracks at the bend.
  • Specifying hardness without the tempering temperature; the same HRC from different tempers behaves differently.
  • Ignoring edge condition; a sheared edge carries micro-cracks into the fatigue section.
  • Assuming annealed strip has no decarburisation; it has to be measured, not assumed.

When A313 wire is the wrong grade

For corrosion or food contact, a stainless spring grade is needed. Above 250 °C the tempered grades sag; use 50CrVA or a stainless spring grade, and design for the loss of load.

Supply range and delivery condition

Table 2 — Supply range by form and delivery condition

Form Size range Condition
Spring wire 0.20–8.00 mm Annealed / hard drawn
Coil 0.20–8.00 mm Bright
A313 wire astm a313 supply range by product form and size
Figure 1 — Supply range by form. Sizes are mill limits, not stock limits.

Chemical composition

Table 3 — Chemical composition (wt. %), balance Fe

Grade C Si Mn Cr Ni Mo
302 ≤0.15 ≤1.00 ≤2.00 17.0–19.0 8.0–10.0 —
304 ≤0.08 ≤1.00 ≤2.00 18.0–20.0 8.0–10.5 —
316 ≤0.08 ≤1.00 ≤2.00 16.0–18.0 10.0–14.0 2.0–3.0

Mechanical properties

Table 4 — Mechanical properties

Grade / temper Tensile Rm Use
302, spring temper 1,600–1,900 MPa General springs
304, spring temper 1,400–1,700 MPa Corrosion + strength
316, spring temper 1,300–1,600 MPa Chloride service

Heat treatment

A313 wire is supplied cold drawn to the spring temper; stress relief after forming is at 250–300 °C. Above 350 °C the cold work is drawn out and the spring loses load.

A313 wire astm a313 property chart
Figure 2 — 302 carries the highest tensile; 316 trades about 300 MPa for chloride resistance.

What ships with every lot

  • EN 10204 3.1 mill certificate with chemistry and mechanical properties
  • Heat number and melt route recorded on the certificate
  • Hardness survey and dimensional report on request
  • Ultrasonic inspection to ASTM A388 / SEP 1921 on request
  • Third-party inspection (SGS, BV, TUV) arranged before dispatch

Packing and delivery

Material is packed for sea freight, marked with grade, heat number, size and net weight; typical lead time 20–30 days from order confirmation.

Table 5 — Trade terms, packing and documents

Item Standard terms
Trade terms FOB Shanghai, Qingdao or Shenzhen; CIF and CFR quoted against the destination port.
Minimum order One bundle or one plate for stock sizes; mill runs and special sections are quoted individually
Lead time 20–30 days from order confirmation for stock sizes; 30–45 days where forging, heat treatment or machining is included
Payment T/T 30 % advance with the order, 70 % against the bill of lading copy; irrevocable L/C at sight accepted for orders above 20 t
Packing Seaworthy export packing — oiled, wrapped, crated or strapped on skids, marked with grade, heat number, size and net weight
Documents 3.1 certificate, packing list, commercial invoice, bill of lading, certificate of origin; legalisation or chamber attestation on request

Frequently asked questions

What does ASTM A313 cover?

Stainless steel spring wire: the grades it includes, the tensile classes and the conditions supplied. It is the standard behind most stainless springs and lockwire.

Which grade should I use for a stainless spring?

302 for general purpose, 304 for better corrosion, 316 for chloride or food service, and 631 (17-7PH) where the spring has to hold load at temperature or after ageing.

What tensile classes are available?

A313 wire is ordered by class rather than by hardness; the class sets the minimum tensile for the diameter. State the class and the diameter, and the certificate reports the measured values.

What lead time applies to ASTM?

20–30 days from order confirmation for stock sizes, 30–45 days where forging, heat treatment or machining is included. Loading from Shanghai, Qingdao or Shenzhen.

Can ASTM be combined with other grades in one shipment?

Yes. Grades that share a heat-treatment and certification route are consolidated into one export package, which is usually what keeps a mixed order economical.

Request a quote

Send these five lines and we quote within one working day

  • Grade and standard
  • Form, size and quantity
  • Delivery condition
  • Certificate and testing requirements
  • Destination port

Email [email protected] or use the form below. Drawings in DXF, STEP or PDF are all fine.

Related grades

Browse all spring steel grades

Governing standard: download the standard (PDF).

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x