ASTM A388 Standard Practice for Ultrasonic Examination of Heavy Steel Forgings

ASTM A388 is the standard practice for ultrasonic examination of heavy steel forgings. It is a practice rather than a specification, which is the single most important thing to understand about it: it tells you how to do the test, not what you have to accept.

What it covers

  • Equipment and probe selection, including frequency ranges for different section thicknesses
  • Calibration against reference blocks and how to set sensitivity
  • Scanning technique and coverage, normally 100 % of the accessible surfaces
  • How to record and size indications
  • Reporting: what the test report must contain

It applies to forgings that are thick enough to need it — typically over 50 mm — and it is usually imposed alongside the material specification, not instead of it.

The part that is negotiated, not specified

A388 does not set acceptance criteria. The buyer and forger agree a quality level — commonly expressed in levels 1 to 4, where 1 is the most stringent — and the acceptance criteria follow from that. This is why an order reading “UT to A388” is incomplete: it describes a competent test with no defined pass mark.

What to put on the purchase order

  • UT to A388 and the acceptance level
  • Whether the test is done on the rough-machined or finished contour
  • Any additional requirement, such as examination from both faces
  • Whether the report has to be witnessed or countersigned

For a critical forging — a pressure-retaining body, a shaft with a fatigue duty — the acceptance level is worth arguing about before the forging is made, not after it is rejected.

Download the standard

ASTM A388 — Ultrasonic examination of heavy steel forgings (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x