ASTM A311 covers cold drawn, stress relieved carbon steel bars subject to mechanical property requirements. It is machining stock: bar that arrives straight, to size, with the internal stress low enough that it does not move when you cut into it.
What it is for
High-volume machined parts — shafts, pins, spacers, bolts — where the bar is turned or milled to final shape and not heat treated afterwards. The stress relief is what stops a long part from bowing when a layer of material is removed from one side.
The classes
| Class | Character | Typical use |
|---|---|---|
| A | Lowest strength, most formable | General machining, light duty |
| B | Intermediate | Shafts and pins with moderate load |
| C | Highest strength of the three | Higher-stress machined parts |
The class sets the mechanical properties; the grade sets the chemistry. Both have to be stated.
What it is not
It is not a heat treatment grade. The bars are stress relieved, not quenched and tempered, and they are not intended for a subsequent hardening operation — the properties are delivered as supplied. If the part has to be hardened after machining, the material should come from a quench and temper specification instead.
What to put on the order
- Grade and class together
- Cold drawn condition, and confirmation that it is stress relieved
- Tolerance and straightness, since these decide whether it runs in a bar feeder
- Whether the part will be machined all over (it usually is)
Getting a copy
The standard is available from ASTM. If you need the mechanical property tables for a specific class, tell us the diameter and the application and we will quote against it.
Related reading
- ASTM A29 — the general requirements these bars are made under.
- Round bar, drill rod and shafting — product forms compared.
- Standards library — the full index.