ASTM A564 2004 Standard Specification for Hot Rolled and Cold Finished Age Hardening Stainless Steel Bars and Shapes

ASTM A564 covers age-hardening (precipitation hardening) stainless steel bars, wire, shapes and forgings. It is the specification behind 17-4PH, 17-7PH and 15-5PH in bar form, and it is unusual because the same grade delivers a wide range of strengths depending on the condition it is supplied in.

What makes this specification different

Most steel standards fix a grade and a heat treatment. A564 fixes a grade and a condition — and the condition is written into the designation. 630 in condition H900 is a different strength from 630 in H1150, and both are compliant with the same standard.

Condition Treatment Character
H900 Age at 480 °C Highest strength, lowest toughness
H1025 Age at 550 °C Balanced
H1150 Age at 620 °C Lower strength, best toughness and corrosion resistance

The grades it covers

630 (17-4PH), 631 (17-7PH), 632, 635, XM-12 (15-5PH), XM-13, XM-14 and others. They are all martensitic or semi-austenitic stainless steels that gain strength from a precipitation reaction during ageing, rather than from a quench.

What to put on a purchase order

  • The grade and the condition — “630 H1150”, not just “630”.
  • Whether the part will be machined before or after ageing — the dimensional change during ageing is small but not zero.
  • Any magnetic or NDT requirement, since these grades are ferromagnetic after ageing.

Download the standard

ASTM A564 — Hot Rolled and Cold Finished Age Hardening Stainless Steel Bars and Shapes (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x