ASTM A242 is the high-strength low-alloy structural steel specified for its atmospheric corrosion resistance. It is the weathering steel of the ASTM family — the grade that forms a stable rust layer instead of continuing to corrode, which is why it is left unpainted on bridges and exposed structures.
What the specification fixes
- Corrosion resistance — at least twice that of carbon structural steel in atmospheric exposure, demonstrated by the accepted copper/alloy content.
- Minimum yield — 345 MPa (50 ksi) at thicknesses up to about 19 mm, tapering in heavier sections.
- Chemistry — copper, chromium, nickel and other additions that drive the oxide layer.
- Forms — plates, bars and shapes for structural use.
When it works and when it does not
The stable patina only forms where the steel stays wet and dry repeatedly, and where it is not exposed to chlorides or trapped moisture. Weathering steel in a marine atmosphere, or in a detail where water sits, corrodes faster than painted carbon steel because there is no coating to protect it. That is a design decision, not a mill decision.
Download the standard
ASTM A242 — High-Strength Low-Alloy Structural Steel (PDF)
Related reading
- Standards library — structural and testing standards in one index.
- Stainless steel corrosion resistance — how alloying changes corrosion behaviour across the families.