ASTM A600 is the specification for high speed tool steel in bar form. It is the document behind a purchase order for M2, M42, T1 or any other M- and T-series high speed steel, and it is the one that decides whether the bar you receive is actually to specification.
What the specification fixes
- Grades — the molybdenum (M) and tungsten (T) high speed steel families, by AISI designation.
- Chemistry — the analysis ranges for carbon, tungsten, molybdenum, vanadium, chromium and cobalt by grade.
- Condition — annealed hardness limits for the delivered bar, and the hardness expected after hardening and tempering.
- Decarburisation — the depth of surface carbon loss permitted, which is what decides whether the bar can be ground to size without losing case.
- Surface and tolerance — the finish and dimensional requirements for hot rolled, cold drawn and ground bar.
Why decarburisation matters
High speed steel is bought for hardness at temperature, and that hardness depends on carbon. A bar that has lost carbon at the surface will not reach the specified hardness after heat treatment, however correct the core analysis is. A600 sets the limit; a mill certificate that omits the decarburisation test is an incomplete certificate.
Download the standard
ASTM A600 (1992) — Standard Specification for High Speed Tool Steel (PDF)
Related reading
- M2 high speed steel bars — the most widely used grade in this specification.
- BS EN ISO 4957 — the European tool steel specification covering the same families.
- Most common tool steel grades — where the high speed group sits against cold work and hot work steels.
- Standards library — every tool steel standard we hold.