BS 970 is the British standard for wrought steels for mechanical and allied engineering purposes. Part 3 covers steels supplied in the bright-drawn, ground or turned condition, and it is the standard behind the EN-series designations that still appear on older drawings: EN8, EN19, EN24, EN36.
Why an obsolete-looking standard still matters
BS 970 was largely superseded by BS EN 10083 and BS EN 10084, but a great many drawings in the UK, India, Southeast Asia and the Middle East still call up EN8 or EN24. When that happens the mill has to translate, and the translation is not always exact.
Reading the designation
The five-digit form encodes the chemistry and the supply condition. For example 817M40 is the modern designation for EN24: the first three digits relate to the composition type, the letter gives the condition (M for mechanical properties, H for hardenability), and the last two give the carbon content in hundredths of a percent (40 = 0.40 % carbon).
| Old designation | Modern | Close to |
|---|---|---|
| EN8 | 212A42 | 1040 / C45 |
| EN19 | 709M40 | 4140 / 42CrMo4 |
| EN24 | 817M40 | 4340 |
| EN36 | 655M13 | Carburising Ni-Cr, similar to 15CrNi6 |
The trap in the translation
“Close to” is not “equal to”. EN24 and 4340 differ in the specified ranges, particularly nickel, and a part designed around one will not necessarily meet its properties in the other. When a drawing cites BS 970, quote against the BS 970 grade, or ask for approval before substituting.
Download the standard
BS 970 Part 3 — Wrought steels in the bright drawn, ground or turned condition (PDF)
Related reading
- AISI 4140 / 42CrMo4 — the equivalent most often quoted against EN19.
- Turned, ground and polished — the supply condition BS 970 Part 3 describes.
- Standards library — the full index.