manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

ASTM A29 Standard Specification Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements

ASTM A29 is the general requirements specification for hot-wrought carbon and alloy steel bars. It is the umbrella document that the individual grade specifications build on, and it is why a bar can be certified to both A29 and, say, A304 at the same time.

What “general requirements” means

A29 does not define a grade. It defines the rules that apply to all hot-wrought bar products: chemical composition limits and how they are determined, permissible variations, dimensions and tolerances, surface quality, decarburisation limits, testing methods, retest procedures and marking.

When a purchase order cites “4140 per A29”, it is buying the grade from the grade specification and the general rules from A29.

What it covers

  • Chemical requirements — product analysis tolerances against the ladle analysis, which is why a certificate can show a carbon figure slightly outside the heat range and still be compliant.
  • Decarburisation — limits on the depth of the soft surface layer, which matters for any part that is machined after heat treatment.
  • Surface quality — what counts as a defect and how much is allowed to be removed.
  • Dimensions and tolerances — by size range and product form.

Where A29 stops

It says nothing about hardenability, mechanical properties or cleanliness — those come from the grade specification (A304 for hardenability bands, A322 for alloy steel bars, A434 for quenched and tempered) or from a separate agreement with the mill.

This is the most common source of confusion: a certificate to A29 alone does not tell you the bar will harden to a given depth, or that it will meet a mechanical property.

Download the standard

ASTM A29 — Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements (PDF)

Related reading

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x