EN 10277 sets the technical delivery conditions for bright steel products — the cold drawn, turned, ground and peeled bars that come out of the mill with a clean surface and a tight tolerance, rather than with scale.
What the standard covers
It defines the product forms and the conditions they are supplied in, plus the surface quality classes that most buyers never specify and then argue about.
| Element | What it fixes |
|---|---|
| Product forms | Cold drawn, turned, ground, peeled, and combinations |
| Delivery conditions | Cold drawn (+C), stress relieved, annealed, quenched and tempered |
| Surface classes | Class A, B and C — from “defects not visible” to “defects permitted within limits” |
| Tolerances | By reference to EN 10278 for dimensions |
| Testing | What must be tested and what the certificate states |
Where it stops
EN 10277 describes the product, not the steel. The grade and its mechanical properties come from the material standard — EN 10083 for quenched and tempered, EN 10084 for case hardening, EN 10088 for stainless. A drawing that cites only EN 10277 has specified a shape and left the material open.
Why the surface class matters
Class A means surface defects are essentially not permitted; class C allows them within stated limits. The price difference between them is real, and so is the risk: a bright bar ordered to class C for a part used as-supplied will show marks that were never screened out. If the drawing is silent, the mill supplies to the default class and the argument happens at goods-in.
What to put on the order
- Grade and material standard (for example 42CrMo4 to EN 10083-3)
- EN 10277 product form and delivery condition
- Surface class, if the surface is functional or visible
- Tolerance class to EN 10278, and straightness
- Whether the bar is machined all over — if it is, do not pay for bright finish
Download the standard
EN 10277 — Bright steel products, technical delivery conditions (PDF)
Related reading
- EN 10278 — the dimensional standard that pairs with this one.
- Turned, ground and polished — what the product forms mean in practice.
- Standards library — the full index.