BS EN ISO 15156-3 is the European adoption of NACE MR0175, part 3 — the section that governs corrosion resistant alloys (CRAs) and other alloys in equipment exposed to hydrogen sulphide during oil and gas production. Part 1 covers general principles, part 2 carbon and low alloy steels, part 3 the CRAs.
Why it matters commercially
In a sour well, the material choice is not a preference — it has to be justified against this standard. A nickel alloy that performs perfectly in sweet service can crack in the presence of H2S, and the specification lays out the limits: partial pressure of H2S, in-situ pH, chloride concentration and temperature. Work outside the qualified envelope and the material is not compliant, whatever the datasheet says.
What part 3 covers
- Stainless steels — martensitic, duplex and austenitic, each with its own environmental limits table.
- Nickel-based alloys — the Inconel, Incoloy and Hastelloy families, qualified by composition and heat treatment.
- Qualification routes — laboratory testing where a material is not listed, and the documentation that testing has to produce.
- Marking and traceability — how a compliant component is identified.
What to send with an enquiry
The H2S partial pressure, the bottom-hole temperature, the chloride level and the pH are what make a grade compliant or not. An enquiry that only says “sour service” cannot be answered with a specific alloy.
Related reading
- Standards library — all the petroleum and alloy standards we work to.
- API 5CRA — the CRA tubular specification that calls up this standard.
- Incoloy 825 — the nickel-iron-chromium alloy commonly specified for sour service.
- Inconel 625 — the higher-strength option where chlorides and H2S combine.