manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Archive for the Industrial Category

Principle and Function of Electroslag Remelting (ESR)

Purpose and Function of Electroslag Remelting As material requirements continue to rise, manufacturers are increasingly focused on not just mechanical strength but also internal cleanliness, microstructural uniformity, and surface finish. This is especially true in critical sectors like aerospace, nuclear, medical, and tooling industries. Recently, customers have

Read more

Lateral Wave Testing Issues and Solutions in Forgings

Surface cracks were visually discovered on wire-cut samples taken from the platform section of aluminum alloy forgings. Metallographic inspection attributed the cracking to excessive residual stress during the cutting process and grain boundary weakening caused by second-phase precipitation. To confirm whether similar defects exist in other forgings,

Read more

Understanding Temper Embrittlement in Steel and Effective Countermeasures

What Is Temper Embrittlement in Steel? Temper embrittlement refers to a phenomenon where quenched steel becomes brittle after tempering within certain temperature ranges or after slowly cooling through these ranges. It can significantly affect the toughness and reliability of steel components. Classification of Temper Embrittlement Temper embrittlement

Read more

Principles and Functions of EAF, AOD, LF, and VD Furnaces

Electric Arc Furnace (EAF) Principle of EAF The Electric Arc Furnace (EAF) primarily relies on the intense heat generated by electric arcs. In the arc zone, temperatures can reach up to 4000°C. The steelmaking process inside an EAF generally includes three stages: Melting phase Oxidation phase Reduction

Read more

Surface Quality Control Measures for Electroslag Remelting Ingots

Background and Significance In recent years, the high-end cast and forged parts market has seen rapid growth, with increasing demand for premium-quality forgings. However, traditional melting and casting techniques often struggle to meet the stringent requirements of advanced forgings, such as bellows, 18-18 retaining rings, and H13

Read more

What Are The Methods For Deburring Parts?

Introduction to Burrs in Metal Processing Burrs are a common issue in metal processing. No matter how advanced or precise your equipment is, burrs often accompany the finished product. They typically form at the edges due to plastic deformation of the material, especially in materials with good

Read more

Influence of Heating Process on Austenite Grain Size in Steel

16MnCr5H is a German-grade steel known for its good hardenability and machinability. After heat treatment, it provides high hardness, strong wear resistance, and good impact toughness at low temperatures. This Mn-Cr alloy steel is widely used in automotive gears for models like Santana, Audi, and Jetta. However,

Read more

6 Key Heat Treatment Questions to Deepen Your Understanding

6 Key Heat Treatment Questions to Deepen Your Understanding 1. What Is Annealing of Steel? What Are Its Types and Applications? Annealing is a heat treatment process in which steel is heated to a temperature above or below its critical point (AC1), held for a specific time,

Read more

Ansteel’s Turbine Steel Used in the “Heart” of the First Domestic F-Class 50MW Heavy-Duty Gas Turbine

  After 13 years of independent research and development, the first domestically produced F-class 50-megawatt heavy-duty gas turbine, known as the “Turbine of National Pride,” was shipped from Deyang, Sichuan, on November 25th, marking its entry into the engineering application phase. This signifies a breakthrough in China’s

Read more

China’s Steel Industry Achieves Breakthrough with Ultra-High Carbon Tool Steel SK120

In August 2024, Chinese steel mills successfully developed and trial-produced the ultra-high carbon tool steel SK120, marking a significant breakthrough in tool steel production. The SK120 product pushed the boundaries of existing steelmaking and hot-rolling production capabilities in terms of carbon content, presenting considerable challenges in trial

Read more

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x