manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

High Speed Steel Circular Saw Blades

Saw blades · Solid HSS, coated HSS and carbide tipped · 160–400 mm

High Speed Steel Circular Saw Blades for Tube and Bar

A solid HSS blade, a coated blade and a carbide-tipped blade cut the same 160–400 mm tube — the difference is how many cuts you get before the blade comes off the machine. We make all three, in M2, M35 and M42 bodies with HSS or carbide teeth, bores from 32 to 50 mm and tooth forms A, B, BW and C to DIN 1838.

160–400 mm
Outside diameter
1.0–3.0 mm
Thickness
32 / 40 / 50 mm
Bore
A / B / BW / C
Tooth form

At a glance

Item Detail
Blade types Solid HSS, coated HSS, carbide tipped — also inserted-tooth and segmental
Body materials DMo5 (M2), Co5 (M35), Co8 (M42); carbide tips on a hardened alloy body
Size range Outside diameter 160–400 mm, thickness 1.0–3.0 mm, bore 32–50 mm
Tooth geometry DIN 1838 form A fine, B coarse, BW and C; 48–100 teeth depending on diameter
Machine fit Pin holes to your spindle — 2/8.5/45, 2/11/63, 4/12/64 and the common circles
Certification EN 10204 3.1 with chemistry and hardness, ISO 9001:2015, AS9120B
Solid HSS, carbide tipped and coated HSS circular saw blades
Solid HSS, inserted carbide tooth and coated HSS blades — the three ways to cut the same bar, side by side.
High speed steel circular saw blade size chart
(a) Blade dimensions: outside diameter against thickness and bore, with the tooth count for each size.
Circular saw blade bore and pin hole options
(b) Bore and pin-hole options — the hole pattern is cut to the spindle, not drilled to a nominal size.
Outside dia D1 (mm) Bore d (mm) Thickness (mm) Teeth, B form
160 32 1.0 – 6.0 48 – 80
200 32 1.0 – 6.0 64 – 100
250 32 1.0 – 6.0 64 – 100
315 40 1.0 – 6.0 80 – 100

DIN 1838 B (coarse tooth, hollow ground). Standard thickness steps: 1.0 / 1.2 / 1.6 / 2.0 / 2.5 / 3.0 / 4.0 / 5.0 / 6.0 mm. Tooth forms A (fine), B, BW and C available; pin holes four or six, or plain bore to drawing.

Chemical component

Supplying size*stocking and accept nonstandard size

*four pin hole, Six pin hole, or client’s request

SurfaceNitride coating (black)Nitride treatment forms a protective layer of Fe304 on the surface of the saw blade through surface treatment, which effectively improves the anti-wear properties of the saw blade and increases its service life for cutting general materials.

Aluminized titanium nitride coating (color)This is a new multi-layer anti-wear coating, recommended for cutting materials with relatively high cutting speed and feed depth and cutting tensile strength over 800N/mm and stainless steel, and for use in particularly harsh working conditions such as dry cutting.

Titanium nitride coating (gold)The main purpose of this coating is to make the saw blade more resistant to cutting, and for general material cutting, its excellent performance can effectively increase the cutting speed and reduce the working loss.

Brown CoatingThis is a high performance PVD coating for severe abrasive wear cutting conditions. Suitable for dry 800n/mm or more high tensile strength materials and stainless steel. Especially for high speed cutting materials and feeds. Coating thickness 0.003 mm.

Super A coatingThe unique Super A coating is mainly suitable for cutting speed higher feed rate conditions, especially for cutting stainless steel and other hard materials, mainly used for dry automobile and motorcycle manufacturing.

Industrial titanium coating (gold color)This is a professional PVD coating resistant to adhesive wear, corrosion and oxidation. It is highly recommended for cutting copper and titanium and has achieved excellent results in cutting off bar, bronze and light alloy operations.

Rose Gold CoatingWith superior high temperature hardness, wear resistance and oxidation resistance, it is especially suitable for high speed milling and dry cutting of various difficult machining materials (Ti, Ai, Ni, Mg alloy, stainless steel).

HSS saw blade also called cold saw, which is designed to cut metal material to transfer the heat generated by cutting to the chips created by the circular saw blade, allowing both the blade and material being cut to remain cool. High speed steel (HSS) saw blade is a kind of blade composed of a certain amount of carbon (C), tungsten (W), molybdenum (Mo), chromium (Cr), vanadium (V), etc. High speed steel blanks, the semi-finished products have high hardness after cutting, forging, annealing, quenching and grinding procedures. Due to the high cutting temperature, however, hardness is still not significantly reduced when it reaches 600 °C or above. The cutting speed can reach more than 60 meters per minute. That the reasons why named high speed steel (HSS) saw blade.

APPLICATIONWhat Materials Do HSS Saw Blade Cut ?HSS circular saw blades are ideal for sawing or cutting off a wide variety of sizes and shapes such as extrusions, tubes, pipes, sheets, plates and some bar stock, including:1 medium to high tensile carbon steel2 sticky materials3 thin walled steel tubes & profiles4 non-alloy tool steel, etc.

CHARACTERISTICSThe Popularity of HSS Saw BladesHSS saw blade can be sharpened with blade sharpening machine or CNC grind machine, which will improve its production efficiency and reduce costs.The popularity of HSS saw blades is increasing because of the technological advancements in grinding machines.HSS saw blades consistently produce the lowest cost per cut among all sawing methods.

APPLICABLE MACHINERYWidely Applied on Pipe Cutting MachinesHigh-speed steel saw blades are widely applied on below machinery:automatic hydraulic pipe cutting machinesemi-automatic hydraulic pipe cutting machinemetal circular saw machinepipe cutting machinepipe processing machinerysawing machinemilling machine, etc.

HSS grade C W V Mo Cr Co
DMo5 (M2 / 1.3343) 0.83–0.88 5.6–6.0 1.75–1.95 4.6–5.0 3.8–4.4 –
Co5 (M35 / 1.3243) 0.83–0.88 5.6–6.0 1.75–1.95 4.6–5.0 3.8–4.4 4.6–4.8
Co8 (M42 / 1.3247) 1.05–1.15 1.15–1.85 0.95–1.35 9.0–10.0 3.5–4.25 7.75–8.75
Outside dia (mm) Thickness (mm) Bore (mm) Pin hole circle (mm) Weight (kg)
200 1.2 / 1.6 / 2.0 32 90 0.3 / 0.4 / 0.5
225 1.2 / 1.6 / 2.0 32 90 0.3 / 0.5 / 0.6
250 1.2 / 1.6 / 2.0 / 2.5 32 / 40 90 0.5 / 0.6 / 0.7 / 0.9
275 1.2 / 1.6 / 2.0 / 2.5 32 / 40 90 0.7 / 0.9 / 1.1 / 1.2
300 1.2 / 1.6 / 2.0 / 2.5 / 3.0 32 / 40 100 0.6 / 0.8 / 1.0 / 1.3 / 1.6
315 1.6 / 2.0 / 2.5 / 3.0 32 / 40 100 0.8 / 1.1 / 1.4 / 1.7
325 1.6 / 2.0 / 2.5 / 3.0 32 / 40 100 0.9 / 1.2 / 1.5 / 1.8
350 2.0 / 2.5 / 3.0 32 / 40 / 50 120 1.5 / 1.8 / 2.0
400 2.0 / 2.5 / 3.0 40 / 50 120 2.0 / 2.5 / 3.0
Bore (mm) Pin hole options (mm)
32 2/8.5/45 · 2/9/50 · 2/11/63 · 2/12/64
40 2/8.5/55 · 2/15/80 · 4/12/64
50 4/15/80 · 4/15/85 · 4/18/100

Three ways to make the same blade

A solid HSS blade is cut from sheet and hardened through, then sharpened. An inserted-tooth blade carries carbide tips on a steel body. A coated blade is HSS with a 2–4 µm layer of TiN or TiAlN on the teeth.

The body is usually the same steel in all three. What changes is the cutting edge — and that is where the cost and the performance sit.

Choosing between them

Blade Speed Life cycle Best for
Solid HSS Moderate Resharpened many times General cutting, low volume, mixed material
Coated HSS Moderate to high Longer between sharpenings; coating lost on regrind Production cutting of steel tube and bar
Carbide tipped High Tips replaced, body lasts High-volume, hard or abrasive material

Why the body matters as much as the teeth

A saw blade is a disc spinning at speed, and the body has to hold the teeth in a straight line without fatiguing. That is why blade blanks are specified for flatness, tensioning and hardness — a blade with good teeth on a badly tensioned body will cut out of square and crack from the rim.

When a blade fails, look at where the crack started. From the rim inward is usually tensioning; from the arbor hole outward is usually a clamping or alignment problem.

What ships with every lot

  • EN 10204 3.1 mill certificate with every blade lot — chemistry, hardness and the heat number
  • Hardness at the tooth root and in the body, reported on the certificate
  • Run-out check on the bore before dispatch
  • Tooth form, pitch and bevel verified against the drawing
  • Hardness traverse across the blade and an edge-angle report, so a regrind starts from a known geometry

Request a quote

Send these five lines and we quote within one working day
  • Standard — Body grade and tooth form — or send the machine model and the cut material
  • Form and size — outside diameter 160–400 mm, thickness 1.0–3.0 mm, bore 32–50 mm
  • Quantity — pieces or kilograms
  • Condition — hardened and tempered; carbide tips brazed and ground
  • Inspection — chemistry, hardness, run-out and a tooth-form drawing

Email [email protected]  or use the form below.

WhatsApp +86 178 7358 1838  ·  Tel +86 731 8990 3933

Related grades

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x