manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Incoloy 800/800H/800HT N08811 N08810 N08800 1.4876 1.4959 Nicekl-Based Alloy

Incoloy 800/800H/800HT N08811 N08810 N08800 1.4876 1.4959 Nicekl-Based Alloy

Incoloy 800800H800HT N08811 N08810 N08800 1.4876 1.4959

Incoloy 800800H800HT N08811 N08810 N08800 1.4876 1.4959

With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

Introduce

Incoloy 800 (UNS N08800, W. Nr. 1.4876) is a widely used material for construction of equipment requiring corrosion resistance, heat resistance, strength, and stability for service up to 1500°F (816°C). Alloy 800 offers general corrosion resistance to many aqueous media and, by virtue of its content of nickel, resists stress corrosion cracking. At elevated temperatures it offers resistance to oxidation, carburization, and sulfidation along with rupture and creep strength.

Application

Incoloy 800 is used in a variety of applications involving exposure to corrosive environments and high temperatures. It is used for heat-treating equipment such as baskets, trays, and fixtures. In chemical and petrochemical processing, the alloy is used for heat exchangers and other piping systems in nitric acid media especially where resistance to chloride stress-corrosion cracking is required. In nuclear power plants, it is used for steam-generator tubing. The alloy is often used in domestic appliances for sheathing of electric heating elements. In the production of paper pulp, digester-liquor heaters are often made of alloy 800. In petroleum processing, the alloy is used for heat exchangers that air cool the process stream.

Standard

Rod, Bar, Wire, Forgings, and Forging Stock: ASTM B 408, ASME SB 408 (Rod & Bar), ASTM B 564, ASME SB 564 (Forgings), ASME Code Case 1325 (All Product Forms), ASME Code Case 1949 (Forgings), AMS 5766 (Rod & Bar), ISO 9723 (Rod & Bar), ISO 9724 (Wire), ISO 9725 (Forgings), BS 3076NA15 (Rod & Bar), BS 3075NA15 (Wire), VdTÜV 412 (All Products).

Plate, Sheet, and Strip: ASTM A 240, ASTM A 480, ASME SA 240, ASME SA 480 (Plate, Sheet, and Strip), ASTM B 409, ASTM B 906, ASME SB 409, ASME SB 906 (Plate, Sheet, and Strip), ASME Code Case 1325 (All Product Forms), ASME Code Case 2339 (Plate), AMS 5871 (Plate, Sheet, and Strip), BS 3072NA15 (Plate & Sheet), BS 3073NA15 (Strip), VdTÜV 412 (All Products), ISO 6208 (plate, sheet and strip).

Pipe and Tubes: ASTM B 163 & ASME SB 163 (Seamless Condenser & Heat Exchanger Tubes), ASTM B 407, ASTM B 829, ASME SB 407, ASME SB 829 (Seamless Pipe & Tubes), ASTM B 514, ASTM B 775, ASME SB 514, ASME SB 775 (Welded Pipe), ASTM B 515, ASTM B 751, ASME SB 515, ASME SB 751(Welded Tubes), ASME Code Case 1325 (All Product Forms), ASME N-20 (Cold Worked Seamless Condenser and Heat Exchanger Tubes for Nuclear Service), BS 3074NA15 (Seamless Pipe & Tubes), VdTÜV 412 (All Products), ISO 6207 (Seamless Tubing).

Other Product Forms:  ASTM B 366 & ASME SB 366 (Fittings)

Chemical Composition

Grade Al C Co Cr Cu Fe Mn N Ni P S Si Ti
Alloy 800 0.3 0.015 0.01 22 0.75 Bal 0.25 0.03 34 0.2 0.02 0.5 0.5

Mechanical Properties

Alloy Form Condition Ultimate

Tensile

Strength,

ksi (MPa)

Yield

Strength

at 0.2%

offset,

ksi (MPa)

Elongation

in 2″

or 4D, percent

800 Sheet, Plate Annealed 85 (586) 40 (276) 43
800 Sheet, Plate

Strip, Bar

Annealed 75 (520)* 30 (205)* 30*
800H Sheet, Plate SHT 80 (552) 35 (241) 47
800H Sheet, Plate

Strip, Bar

SHT 65 (450)* 25 (170)* 30*

Machinability

Machining characteristics of this INCOLOY alloy 800 are similar to that of iron-based alloys. This alloy tends to work-harden during machining.

Welding

INCOLOY alloy 800 can be welded by common welding techniques, using a matching filler metal.

Forming

This alloy exhibits good ductility and hence can be formed using conventional methods.

Hot working

INCOLOY alloy 800 can be hot worked at temperature ranges of 871-1232°C (1600-2250°F).

Cold Working

Cold working may be done on the alloy using standard tooling.

Annealing

INCOLOY alloy 800 may be annealed after cold working. Annealing should be done at 982°C (1800°F) for 15 min and then the alloy should be air cooled.

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x