M2 High Speed Steel Strip For Blade

M2 High Speed Steel Strip For Blade

SK5 SK85 JIS Carbon Tool Steel

High speed special tool steel

M2 High Speed Steel Strip For Blade steel (otherwise W6Mo5Cr4V2  or the same as 1.3343) is a high speed steel in tungsten-molybdenum series.

 

The carbides in it are small and evenly distributed. It has high wear resistance. After heat treatment, its hardness is the same as T1, but its bending strength can reach 4700 MPa, and its toughness and thermoplasticity are higher than T1 by 50%.

 

It is usually used to manufacture a variety of tools, such as drill bits, taps and reamers.

 

Application

  1. Gear Cutter
  2. Hacksaw blade
  3. Saw blades
  4. Slitting saw
  5. Circular saw blade
  6. Cutting blade
  7. Power planner replaceble blade
  8. Sugar cane juice extractor blade

 

Specification

Steel Grade: M2, M35, M40 , M42 etc (usually )

Delivery status: annealed, quenched, tempered

Surface: black, grinding, polishing, bright

High-Speed Steel Strip Dimensions

Premium high-speed steel strips engineered for precision cutting tools and industrial applications. Featuring excellent hardness, wear resistance, and heat stability for demanding machining environments.

Parameter Range
Thickness 0.6 – 8 mm
Width 5 – 35 mm

 

M2 Steel Chemical Composition

Grade C Si Mn P S Cr Mo W V
M2 0.86-0.94 0.45max 0.4max 0.03max 0.030max 3.8-4.5 4.7-5.2 5.9-6.7 1.7-2.4

 

M2 Steel Properties Mechanical

Mechanical properties Metric Imperial
Hardness, Rockwell C (tempered at 1150°F, quenched at 2200°F) 62 62
Hardness, Rockwell C (as hardened, quenched at 2200°F) 65 65
Compressive yield strength (when tempered at 300°F) 3250 MPa 471000 psi
Izod impact unnotched (when tempered at 300°F) 67 J 49.4 ft-lb
Abrasion (loss in mm3, as-hardened; ASTM G65) 25.8 25.8
Abrasion (loss in mm3, tempered at 1275°F; ASTM G65) 77.7 77.7
Poisson’s ratio 0.27-0.30 0.27-0.30
Elastic modulus 190-210 GPa 27557-30458 ksi

 

 

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x