With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

Introduction

Nickel 201 alloy is a commercially pure wrought alloy having properties similar to that of nickel 200 alloy, but with a lower carbon content to avoid embrittlement by inter-granular carbon at high temperatures.

It is resistant to acids and alkalis, and dry gases at room temperature. It is also resistant to mineral acids depending on the temperature and concentration of the solution.

 

Chemical Composition

The chemical composition nickel 201 alloy is outlined in the following table.

Element Content (%)
Nickel, Ni ≥ 99
Iron, Fe ≤ 0.4
Manganese, Mn ≤ 0.35
Silicon, Si ≤ 0.35
Copper, Cu ≤ 0.25
Carbon, C ≤ 0.020
Sulfur, S ≤ 0.010

 

Physical Properties

The following table shows the physical properties of nickel 201 alloy.

Properties Metric Imperial
Density 8.89 g/cm3 0.321 lb/in3
Melting point 1435 – 1446°C 2615 – 2635°F

 

Mechanical Properties

The mechanical properties of nickel 201 alloy are displayed in the following table.

Properties Metric Imperial
Tensile strength (annealed) 403 MPa 58500 psi
Yield strength (annealed) 103 MPa 14900 psi
Elongation at break (annealed prior to test) 50% 50%

Thermal Properties

The thermal properties of nickel 201 alloy are given in the following table

Properties Metric Imperial
Thermal expansion co-efficient (@20-100°C/68-212°F) 13.1 µm/m°C 7.28 µin/in°F
Thermal conductivity 79.3 W/mK 550 BTU.in/hrft².°F

 

Other Designation

Other designations that are equivalent to nickel 201 alloy include the following:

ASME SB-160 – SB 163

SAE AMS 5553

DIN 17740

DIN 17750 – 17754

BS 3072-3076

ASTM B 160 – B 163

ASTM B 725

ASTM B730

 

Applications

The following are the list of applications of nickel 201 alloy:

Caustic evaporators

Combustion boats

Electronic components

Plater bars.

 

Overview

Commercially pure wrought Nickel with similar properties to Alloy 200 but with a lower carbon content to prevent embrittlement by inter-granular carbon at elevated temperatures.

 

Characteristics

Good resistance to corrosion in acids and alkalis and is most useful under reducing conditions.

Outstanding resistance to caustic alkalis up to and including the molten state.

In acid, alkaline and neutral salt solutions the material shows good resistance, but in oxidising salt solutions severe attack will occur.

Resistant to all dry gases at room temperature and in dry chlorine and hydrogen chloride may be used in temperatures up to 550C.

Resistance to mineral acids varies according to temperature and concentration and whether the solution is aerated or not. Corrosion resistance is better in de-aerated acid.

Virtually immune to inter granular attack above 315C, chlorates must be kept to a minimum.

 

Nickel 201 can be hot formed to almost any shape. The temperature range 1200°F to 2250°F is recommended and should be carefully abided as the proper temperature is the most important factor in achieving hot malleability. Full information of the forming process should be sought and understood before proceeding.

 

Nickel 201 can be cold formed by all conventional methods, but because nickel alloys have greater stiffness than stainless steels more power is required to perform the operations.

Nickel 201 is the low carbon version of Nickel 200. It is preferred to Nickel 200 for applications involving exposure to temperatures above 600°F. With low base hardness and lower work-hardening rate, it is particularly suited for cold forming.

 

Nominal Mechanical Properties of Nickel 201
Form Condition Tensile
Strength
Kpsi
Yield Strength
(0.2% Offset)
Kpsi
Elongation
in 2″ (%)
Hardness
Rod and Bar Hot Finished,
Hot Finished
and Annealed
50-60 10-25 60-40 75-100 Brinell
Cold Drawn 60-100 35-90 35-10 125-200 Brinell
Cold Drawn
and Annealed
50-60 10-25 60-40 75-100 Brinell
Plate Hot Rolled 50-70 12-25 60-35 —
Hot Rolled
and Annealed
50-70 12-35 60-40 —
Tube and Pipe* Cold Drawn
Annealed
50-70 10-28 60-40 62 Max
Rockwell B
Stress Relieved 60-105 30-85 35-15 70-95
Rockwell B

 

High Temperature Mechanical Properties of Annealed Nickel 201
Temp.°F Tensile Strength, PSI Yield Strength, PSI Elongation,% Reduction of Area, %
Room 58,500 15,000 50 73
200 56,100 15,400 45 74
400 54,000 14,800 44 72
600 52,500 15,300 42 72
800 41,200 13,500 58 80
1000 33,100 12,100 60 84
1200 22,200 10,200 74 90

 

INTERNATIONAL STANDARDS
Country Material Pipe/Tube Sheet/Plate Bar/Rod Fitting Forging
USA ASTM UNS N02201 B161 B162 B160 B366 B564
Germany DIN 2.4068 17751 17750 17752 – 17754
UK BS NA 12 3074 3072 3076 – –

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x