manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Stainless Steel Welding Wire

Stainless Steel Welding Wire

Introduce

Our stainless steel welding wire is produced to the highest quality standards to ensure ease of use and consistency.

Leading Stainless Steel Welding Wire Manufacturer

  1. Professional Stainless Steel Welding Wire Experience
  2. Wide Options For Your Unique Stainless Steel Welding Wire
  3. Original Manufacturer with Competitive Price

 

For Stainless Steel Welding Wire Manufacturers & Suppliers

Our in-house modern production plant allows us to offer great quality options to appeal to your target customers. Our streamlined manufacturing processes are here to provide you with the best stainless steel welding wire in the market.

 

For Stainless Steel Welding Wire Wholesalers

Being one of the most equipped stainless steel welding wire manufacturing companies, we offer the best quality products at a significantly low cost. This allows us to work with you to ensure that you get to also extend great prices to your customers.

 

For Stainless Steel Welding Wire Brand Owners

We have worked with different businesses taking their ideas from conception to fulfilling their desired stainless steel welding wire solutions. Help you better define what you want and realize your brand’s product solutions.

 

Stainless Steel Welding Wire Features

  • Welding alloy welding stainless steel mig welding wire
  • Designed for welding heat treatable base alloys
  • Higher melting point and more fluidity
  • Suitable for sustained elevated temperature service
  • All position, include vertical down welding
  • Gray – white(post anodized) color

 

Stainless Steel Welding Wire Application

Welding stainless steel wire is used in the welding of similar base materials, equipment and machine parts that require good comprehensive performance, furniture decoration and food medical industry.

 

Choose Your Stainless Steel Welding Wire

  • MIG Wire Size

mm: 0.8mm / 0.9mm / 1.0mm / 1.2mm/ 1.6mm

inch: 0.030 / 0.035 / 0.040 / 0.045/ 3/16 – 3/64

  • Spool Weight(Package)

0.5kg / 2kg / 7kg

  • Brush Welding Size

mm: 1.2mm/ 1.6mm/ 2.0mm/ 2.4mm/ 3.2mm/ 4.0mm

  • Weight(Package)

5kg / 10kg / 1LB / 2LB / 4.5LB / 20LB

 

308L ER308L For low carbon 18Cr-8Ni stainless such as ISI 304
308H ER308H Suitable for welding AISI 304 and 308H steel, good strength at high temperature due to higher carbon content.
308LSi ER308LSi Weldability and fluidity are better than 308L, Good crack and corrosion resistance due to moderate ferrite content.
316L ER316L A general purpose wire for welding AISI 316L, and equivalent grades.
316LSi ER316LSi A general purpose wire for welding AISI 316L, and equivalent grades. High silicon content for minimal spatter and weld metal fluidity.
309L ER309L Good crack and corrosion resistance due to moderate ferrite content, superior corrosion at 90c due to more Ni and Cr content.
309LSi ER309LSi Weldability and fluidity are better than 309L
310 ER310 A 25%Cr 20% Ni wire for welding AISI 310s steels and dissimilar metals, also suitable for non magnetic application.
347Si ER347Si A general purpose wire for welding AISI321, 347, and equivalent grades, High silicon content for minimal spatter, and weld fluidity.
312 ER310 For 29 Cr-9Ni stainless steels, dissimilar metal welding, it is suitable for, clad steel, stainless steel sheet linings, alloy steel with high hardenability and used as buffer layer before hardfacing.
2209 ER2209 A Duplex type stainless steel wire, used for welding 22CR/9Ni type materials, higher strength and excellent resistance to pitting and stress corrosion cracking.
2594 ER2594 A Super Duplex type wire used for welding of 25/10/5 material.

 

Details Of Stainless Steel Welding Wire

Type Chemical Composition
AWSA5.1 AWS A5.1M C Mn Si P S Ni Cr Mo V
E6011
E6013
E4311
E4313
≤0.20 ≤1.20 ≤1.00 … … ≤0.30 ≤0.20 ≤0.30 ≤0.08
E7016
E7018
E4916
E4918
≤0.15 ≤1.60 ≤0.75 ≤0.035 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
E7018M E4918M ≤0.12 0.40~1.60 ≤0.80 ≤0.030 ≤0.020 ≤0.25 ≤0.15 ≤0.35 ≤0.05
E308-16
E308L-16
E308-17
E308L-17
≤0.08 0.50~2.50 ≤1.00 ≤0.04 ≤0.03 9.0~11.0 18.0~21.0 ≤0.75 Cu ≤0.75
≤0.04
E309 -16
E309L-16
E309-17
E316-17
≤0.15 0.50~2.50 ≤1.00 ≤0.04 ≤0.03 12.0~14.0 22.0~25.0 ≤0.75 Cu ≤0.75
≤0.04
E316-16
E316-16
E316L-17
E309L-17
≤0.08 0.50~2.50 ≤1.00 ≤0.04 ≤0.03 11.0~14.0 17.0~20.0 2.0~ 3.0 Cu ≤0.75
≤0.04
E312-16 E312-17 ≤0.15 0.50~2.50 ≤1.00 ≤0.04 ≤0.03 8.0~10.5 28.0~32.0 ≤0.75 Cu ≤0.75
Note: E7016 and E7018 components of Mn+Ni+Cr+Mo+VS1.75;stainless steel electrode code
interpretation – example E308-XX (E308-15/E308-16/E308-17/E308-26……), the prefix code isdivided into -1/-2/-4, representing the welding position; the suffix code is divided into -5l-6/-7,in which 5 represents the alkalinity, 6 represents rutile,and 7 represents the titanic acid type.

 

Type Mechanical Properties
AWSA5.1 AWS A5.1M Tensile Strength Mpa Yield Strength Mpa Elongation A (%) Impact Value Radio graphics
KV2(J) -45℃ KV2 ()-30℃
E6011 E4311 ≥430 ≥330 ≥22 … ≥ 27 Grade ll
E6013 E4313 ≥430 ≥330 ≥17 … …
E7016 E4916 ≥490 ≥400 ≥22 ≥ 27 ≥ 27 Grade l
E7018 E4918 ≥490 ≥400 ≥22 ≥ 27 ≥ 27
E7018M E4918M Normal ≥ 490 370~500 ≥24 … ≥ 67
2.4MM/370~530
E308-XX ≥550 ≥30
E308L-XX ≥520
E309-XX ≥550
E309L-XX ≥520
E316-XX ≥520
E316L-XX ≥490
E312-XX ≥ 660 ≥22
Note: E6011 has no special requirements for heat preservation furnace and drvina: Environmental temperature: 20~ 40 C;The requirement of E6013 heat preservation furnace is higher than theambient temperature [10C ~20C];Drying requires drying at least 1 hour at 120 C150 C;E7016/E7018/E7018M requirements for heat preservation furnace and drying; Environmentaltemperature: [30C~140C];Drying requires drying at least 1~2 hours at 260℃~425℃;

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x