manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

WHAT IS TEMPERING?

WHAT IS TEMPERING?

Tempering is a heat treatment process that alters the mechanical properties (typically ductility and hardness) and relieves internal stresses of a steel. Tempering allows carbon trapped in a martensitic microstructure to disperse, and enables the internal stresses to be released from the steel that may have been created from prior operations.

 

How a plain carbon steel and an alloy steel respond to the same tempering temperature.
Figure 1: How a plain carbon steel and an alloy steel respond to the same tempering temperature.

The Tempering Process

Tempering is performed by elevating the steel to a set point below its lower critical temperature, typically following a hardening operation. Once this temperature is reached, it is held there for a specified amount of time. The exact temperature and time depend on several factors such as the type of steel and desired mechanical properties.

 

To get the steel to its critical temperature, some type of heating device must be used. Common devices include gas furnaces, electrical resistance furnaces, or induction furnaces. Often, this heating is done in a vacuum or with an inert gas to protect the steel from oxidation. Once the furnace achieves the desired temperature, a dwell time occurs. Following the dwell time, the furnace is shut off and the steel is allowed to cool at predetermined rate.

 

Why Is Steel Tempered?

Tempering steel after a hardening process allows for a middle ground of hardness and strength. This is achieved by allowing the carbon diffusion to occur within a steel microstructure. When steel is hardened, it can become excessively brittle and hard. However, when not hardened, the steel may not have the strength or abrasion resistance needed for its intended application. Tempering also improves the machinability and formability of a hardened steel, and can reduce the risk of the steel cracking or failing due to internal stresses.

 

When Is Tempering Used?

Tempering is most commonly used following a quenching operation. Heating a carbon steel and rapidly quenching it can leave it too hard and brittle. Tempering it can restore some of its ductility.

Tempering can reduce the hardness and relieve the stress of a welded component. Welds can create a localized zone that has been hardened due to the heat of the welding process. This can leave undesirable mechanical properties and residual stress that can promote hydrogen cracking. Tempering helps prevent this.

Work hardened materials often require tempering. Materials can become work hardened through processes such as punching, bending, forming, drilling, or rolling. Work hardened materials have a high amount of residual stresses that can be alleviated through a tempering process.

 

Fushun Special Steel LTD CO

Fushun Metal is a large special steel manufacuter and supplie. We are metal experts and have been providing quality customer service and products since 1998.

 

At Fushun Metal, we supply a wide range of metals for a variety of applications. Our products/stock includes: stainless steel, alloy steel, spring steel, tool steel, high speed steel, mould steel, nickel alloy.

 

Our hot rolled and cold rolled steel is available in a wide range of shapes including: bars, tubes, sheets and plates. We can cut metal to your exact specifications.

 

Send your inquiry information to us and get a free quotation today!

What tempering is for

Tempering is the step after quenching, and its job is to give back some of the toughness the quench took away. As-quenched martensite is hard and brittle; heating it to a temperature below the critical range lets the carbon diffuse out of supersaturation, relieving internal stress at the cost of some hardness.

Every tempering temperature is a point on a trade curve: higher temperature buys toughness and gives up hardness. The whole skill is choosing that point, and choosing it deliberately rather than by habit.

Why alloy steels behave differently

A plain carbon steel falls steadily as the tempering temperature rises. An alloy steel does not: after a dip, its hardness climbs again around 500 °C as fine alloy carbides precipitate, then falls away above about 600 °C.

That second peak is why the same temper can produce a harder part in a Cr-Mo steel than in a carbon steel — and why copying a tempering temperature from one grade to another is unsafe.

The range to avoid

Between roughly 250 and 400 °C many steels lose hardness without gaining useful toughness. Parts tempered in that window tend to chip, and the certificate still shows an acceptable hardness number, which makes the failure hard to trace.

Two sensible windows: low temper (150–250 °C) for wear resistance, or high temper (500–650 °C) for toughness at moderate hardness.

Practical rules

  • Temper immediately after quenching — a quenched part left overnight can crack on its own.
  • Temper twice on alloy and tool steels; the second pass converts retained austenite.
  • Soak long enough for the centre to reach temperature, roughly one hour per 25 mm of section.
  • Never temper at a temperature the drawing does not allow, even to “make the hardness fit”.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x