What is the Difference Between Inconel and Incoloy?

Although Inconel® and Incoloy® belong to the same family of superalloys, each possesses its own distinct properties, as well as sharing others. Also known as high-performance alloys, the superalloys in general provide high resistance to corrosion and oxidation, as well as mechanical strength at elevated temperatures.
The most fundamental of difference between them lies in their composition. Inconel®, predominantly of nickel-chrome, generally contains over 50% nickel, whereas Incoloyl®, a nickel-iron-chromium alloy, has less than 50% nickel content.
On a more specific level, the major distinctions between the two are their applications and spheres of suitability.
Inconel®
Inconel®, when heated, forms a thick yet stable oxide layer that protects its outer surface from further attack. This makes it the ideal choice for extreme temperature and pressure applications, where steel and aluminum would succumb to thermal creep. Available in numerous grades, the Inconel® alloys exhibit shifting characteristics with slight variations in their chemistry.
In its more basic form, typical applications would include the food industry and heat treatment components. When alloyed with other elements, however, further strengthening and stiffening permits its use in the more demanding areas of the marine, aerospace and chemical processing industries. Alloyed to its peak performance, Inconel then becomes the material of choice in the most critical environments of turbine blades, rocket engines and key nuclear industry components.
Incoloy®
Incoloy®, with its higher ferrous content and correspondingly lower cost, make it the ideal material in elevated temperature, but less critical, applications. A further feature is its relative ease of fabrication, employing the same machines and processes used for stainless steel.
This alloy also comes in a variety of grades, whose emphasis is more on resistance to aggressive forms of corrosion, particularly in aqueous environments. Whereas a basic form of Incoloy will find widespread general use, further alloying with enhancing elements provides added resistance to chemical and environmental corrosion, as well as physical deterioration, such as surface pitting and cracking.
Excellent resistance to seawater, brine, sour gas and high chloride environments make it a popular choice in the oil and gas industries. The most specialized Incoloy® alloys, however, are widely used in the harshest chemical environments of all, involving among others, acids, wet scrubbing, nuclear fuel and the reactive atmospheres of furnaces.
Fushun Special Steel LTD CO
Fushun Metal is a large special steel manufacturer and supplier. We are metal experts and have been providing quality customer service and products since 1998.
At Fushun Metal, we supply a wide range of metals for a variety of applications. Our products/stock includes: stainless steel, alloy steel, spring steel, tool steel, high speed steel, mould steel, nickel alloy.
Our hot rolled and cold rolled steel is available in a wide range of shapes including: bars, tubes, sheets and plates. We can cut metal to your exact specifications.
Send your inquiry information to us and get a free quotation today!
The difference is iron, not quality
Inconel and Incoloy are both nickel superalloy families from the same producer, and neither name describes a grade. The dividing line is composition: Inconel grades are nickel-based, with iron kept low; Incoloy grades are nickel-iron, with iron forming the balance.
That single difference decides almost everything else — how much the alloy costs, how well it holds strength at temperature, and where it should not be used.
Where each one belongs
| Need | Grade | Why |
|---|---|---|
| Strength above 700 °C | Inconel 718, X-750 | Age-hardened nickel base holds its structure |
| Oxidation at 1,100 °C | Inconel 601 | Chromium plus aluminium forms a tenacious oxide |
| Seawater, acid, chloride SCC | Inconel 625, Incoloy 825 | Molybdenum plus high nickel |
| Furnace tube, reformer | Incoloy 800H | Creep strength at a fraction of the cost |
The mistake buyers make
Specifying Inconel where Incoloy would do. Both resist chloride stress corrosion cracking, both are austenitic and non-magnetic, and both weld the same way. If the service temperature is under about 650 °C and the duty is corrosion rather than creep, an Incoloy 825 will usually perform for a materially lower price per kilogram.
The reverse error is rarer but more expensive: Incoloy in a high-temperature load-bearing application, where it creeps and the part distorts long before it was expected to fail.