1.2516 120WV4 Cold Working Tool Steel

1.2516 120WV4 Cold Working Tool Steel

120WV4 1.2516 Cold Working Tool Steel

1.2516 120WV4 Cold Working Tool Steel

1.2516 Introduction:

Low alloyed W cold working tool steel.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

1.2516 Applications:

Twist drills and tapes, ejectors, punches, reamers, countersinks, engraving tools, metal cutting saws. Usually delivered as silver steel.

3 Quality Standard:

BS EN ISO 4957 Tool Steel

4 All Grades Comparison:

Material No. EN
1.2516 120WV4

5 Chemical Composition(%)

C Si Mn P S Cr W V
1.15-1.25 0.15-0.30 0.20-0.35 0.035 max 0.035 max 0.15-0.25 0.90-1.10 0.07-0.12

6 HEAT TREATMENT:

  • SOFT ANNEALING: Heat to 720-750oC, cool slowly in furnace. This will produce a maximum Brinell hardness of 230.
  • STRESS RELIEVING:Stress relieving to remove machining stresses should be carried out by heating to approx. 650oC, holding for 1-2 hours at heat, followed by air cooling. This operation is performed to reduce distortion during heat treatment.
  • HARDENING:Harden from a temperature of 760-820oC, 800-840oC followed by water or oil quenching. Hardness after quenching is 64-66 HRC.
  • TEMPERING: Tempering temperature: 150-250oC. See the data bellow.
Tempering Temperature Hardness(HRC)
100oC 66
200oC 65
300oC 59
400oC 53

7 1.2516 Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x