manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

1.4913 (X19CrMoNbVN11-1) Heat Resistant Steel

 

1.4913 (X19CrMoNbVN11-1) Heat Resistant Steel

Professional Steel Manufacturer – FUSHUN SPECIAL STEEL

Steel Grade Introduction and Applications

FUSHUN SPECIAL STEEL specializes in manufacturing 1.4913 (X19CrMoNbVN11-1) heat resistant steel, a premium high-temperature heat-treatable steel engineered for demanding industrial applications. This advanced steel grade incorporates boron and nitrogen alloying elements to achieve exceptional creep rupture strength and corrosion resistance at elevated temperatures up to 600°C.

As a leading steel manufacturer, FUSHUN SPECIAL STEEL provides 1.4913 steel for critical applications including thermal power generation components, high-temperature fasteners, turbine blades, steam valves, and precision shafts. Our manufacturing expertise ensures consistent quality and reliable performance in high-stress, high-temperature environments.

We welcome large-volume orders and provide comprehensive manufacturing solutions for industrial clients worldwide.

Chemical Composition

Element C Si Mn Cr Ni Mo V Nb
Min % 0.17 0.10 0.40 10.00 0.30 0.50 0.10 0.05
Max % 0.22 0.50 0.80 11.50 0.60 0.80 0.30 0.55

FUSHUN SPECIAL STEEL maintains strict quality control to ensure precise chemical composition meeting international standards.

Available Processing Types

Hot Rolled

FUSHUN SPECIAL STEEL provides hot rolled 1.4913 steel with excellent surface quality and dimensional accuracy. Our hot rolling process ensures optimal microstructure for superior mechanical properties.

Hot Forged

Our advanced forging capabilities produce high-strength 1.4913 components with refined grain structure and enhanced mechanical properties for critical applications.

Available Shapes and Forms

Round Bars

Precision round steel bars for shafts and fasteners

Flat Bars

High-quality flat steel for various applications

Plates

Steel plates for structural components

Tubes

Seamless tubes for high-pressure applications

Size Capabilities and Dimensions

Hot Rolled Rounds

Maximum diameter: 260mm

Precision tolerance and excellent surface finish

Forged Products

Maximum diameter: 1200mm

Large-scale forging capabilities for critical components

Precision Machining

Ultra-precise dimensions available

In-house turning and grinding capabilities

Mechanical Properties

Condition Diameter (mm) Yield Strength (N/mm²) Tensile Strength (N/mm²) Elongation (%) Impact Toughness (J)
+QT ≤ 160 ≥ 750 900 – 1050 ≥ 12 ≥ 20

High Temperature Performance

Temperature (°C) Minimum Yield Strength (N/mm²)
350 ≥ 610
600 ≥ 305

Heat Treatment Capabilities

Quenching & Tempering (+QT)

Hardening: 1100-1130°C

Tempering: 670-720°C (min 2h)

Cooling: Oil, polymer, or air

Stress Relieving (+SR)

Temperature: 630-710°C

Cooling: Air

Reduces internal stresses

FUSHUN SPECIAL STEEL operates in-house heat treatment facilities ensuring consistent quality and fast delivery times.

FUSHUN SPECIAL STEEL Manufacturing Advantages

In-House Heat Treatment

Complete heat treatment facilities ensure stable quality control and faster delivery times for all orders.

Precision Machining

Advanced turning and grinding capabilities reduce downstream processing time and costs for customers.

Large Volume Manufacturing

As a professional steel manufacturer, we welcome large-scale orders with competitive pricing and reliable delivery.

Quality Assurance

Comprehensive testing and quality control systems ensure consistent material properties and performance.

Contact FUSHUN SPECIAL STEEL today for your 1.4913 steel requirements. We specialize in large-volume manufacturing with superior quality and competitive delivery times.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x