BS EN 10084 sets the technical delivery conditions for case-hardening steels. It is the European standard behind 16MnCr5, 20MnCr5, 18CrNiMo7-6 and 15CrNi6, and it is what a carburising grade should be ordered against in Europe.
What the standard fixes
- Chemical composition — the ranges for each grade, with tighter limits than a mill’s internal aim.
- Two quality classes — the standard distinguishes grades by hardenability control, which decides whether the steel behaves predictably in a carburising furnace.
- Grain size — fine grain is specified, because a coarse-grained case becomes brittle.
- Delivery condition — usually annealed for machining, with a hardness ceiling.
- Testing and marking — what the certificate must state.
The grades and what they are for
| Grade | Character | Typical use |
|---|---|---|
| 16MnCr5 | The workhorse, cheap and adequate | General gears and shafts |
| 20MnCr5 | Higher carbon, better core strength | Larger sections |
| 15CrNi6 | Nickel for core toughness | Shock-loaded gears |
| 18CrNiMo7-6 | High hardenability and toughness | Large transmission parts, wind turbine gears |
What to specify beyond the grade
The case depth and the surface hardness after heat treatment, plus the core hardness required. Those three are not in EN 10084 — the standard stops at the steel, and the treatment is the buyer’s specification.
Download the standard
BS EN 10084 — Case hardening steels, technical delivery conditions (PDF)
Related reading
- 16MnCr5 / 1.7131 — the most widely used grade in this standard.
- 1.5919 / 15CrNi6 — the nickel-bearing option for tough cores.
- Standards library — the full index.